General
Property | Value |
---|---|
Huella de carbono | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Medidas
Property | Value |
---|---|
Longitud | 400 - 7000 mm Show Supplier Material materials with Longitud of 400 - 7000 mm |
Dimensions | Diameter = 152 mm (6”), 178 mm (7”), 203 mm (8”), 228 mm (9”), 254 mm (10”), 279 mm (11”), 306 mm (12”), 356 mm (14”), 406 mm (16”), 457 mm (18”). |
Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia a la tracción | 23.0 °C | 283 - 294 MPa Show Supplier Material materials with Resistencia a la tracción of 283 - 294 MPa |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 607 - 657 °C Show Supplier Material materials with Temperatura de fusión of 607 - 657 °C | Solidus (607-619°C); Liquidus (655-657°C) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | according to EN 573-3 | |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % | according to EN 573-3 | |
Hierro | 0.35 % Show Supplier Material materials with Hierro of 0.35 % | according to EN 573-3 | |
Magnesio | 0.4 - 0.6 % Show Supplier Material materials with Magnesio of 0.4 - 0.6 % | according to EN 573-3 | |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % | according to EN 573-3 | |
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | according to EN 573-3 | |
Silicona | 0.6 - 0.9 % Show Supplier Material materials with Silicona of 0.6 - 0.9 % | according to EN 573-3 | |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | according to EN 573-3 | |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % | according to EN 573-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Extrusion Applications | |
Processing history | Smelters: Sayanogorsk Aluminium Smelter (SAZ), Krasnoyarsk Aluminium Smelter (KRAZ), Kubikenborg Aluminium AB (KUBAL) |