General
Property | Value |
---|---|
Huella de carbono | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Medidas
Property | Value |
---|---|
Dimensions | 9,5 mm, 12 mm, 15 mm, 19 mm, 25 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia a la tracción | 23.0 °C | 80 - 95 MPa Show Supplier Material materials with Resistencia a la tracción of 80 - 95 MPa |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 660 °C Show Supplier Material materials with Temperatura de fusión of 660 °C | approximate |
Eléctrico
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 61.9 % IACS Show Supplier Material materials with Specific Electrical conductivity of 61.9 % IACS | min |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Electric conductors and cables, multi-void conform extrusions | |
Processing history | Smelters: Irkutsk Aluminium Smelter (IrKAZ), Kandalaksha Aluminium Smelter (KAZ), Bratsk Aluminium Smelter (BrAZ) |