General
Property | Value |
---|---|
Huella de carbono | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Medidas
Property | Value |
---|---|
Dimensions | Cross section: 500x2130 mm, 560x1100 mm, 560x1230 mm, 560x1310 mm |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Cobre | 0.15 % Show Supplier Material materials with Cobre of 0.15 % | according to DIN EN 573-3 | |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % | according to DIN EN 573-3 | |
Hierro | 0.35 % Show Supplier Material materials with Hierro of 0.35 % | according to DIN EN 573-3 | |
Magnesio | 4 - 5 % Show Supplier Material materials with Magnesio of 4 - 5 % | according to DIN EN 573-3 | |
Manganeso | 0.2 - 0.5 % Show Supplier Material materials with Manganeso of 0.2 - 0.5 % | according to DIN EN 573-3 | |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % | according to DIN EN 573-3 | |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % | according to DIN EN 573-3 | |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | according to DIN EN 573-3 | |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % | according to DIN EN 573-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Aluminium can end | |
Processing history | Smelters: Bratsk Aluminium Smelter (BrAZ) |