General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 2.5 - 2.6 g/cm³ Show Supplier Material materials with Densidad of 2.5 - 2.6 g/cm³ | approx. |
Porosidad | 0 % Show Supplier Material materials with Porosidad of 0 % | approx., ISO 9385 |
Medidas
Property | Value |
---|---|
Ancho | 900 - 1100 mm Show Supplier Material materials with Ancho of 900 - 1100 mm |
Espesor | 3 - 6 mm Show Supplier Material materials with Espesor of 3 - 6 mm |
Longitud | 1600 - 1954 mm Show Supplier Material materials with Longitud of 1600 - 1954 mm |
Dimensions | Flat cut-to-size panels and bent panels are also available. Formats of flat cut-to-size panels and bent panels on request. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.25 - 0.26 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.25 - 0.26 [-] | approx., ASTM C-1259 |
Dureza Knoop HK2 | 20.0 °C | 570 - 600 [-] Show Supplier Material materials with Dureza Knoop HK2 of 570 - 600 [-] | approx., ISO 9385 (HK 0.1/20) |
Módulo elástico | 20.0 °C | 84 - 95 GPa Show Supplier Material materials with Módulo elástico of 84 - 95 GPa | approx., ASTM C-1259 |
Resistencia a la flexión | 20.0 °C | 100 - 165 MPa Show Supplier Material materials with Resistencia a la flexión of 100 - 165 MPa | approx., DIN EN 1288, Part 5, R45 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 800 - 850 J/(kg·K) Show Supplier Material materials with Calor específico of 800 - 850 J/(kg·K) | for 20-100°C |
Coeficiente de dilatación térmica | 50.0 °C | -8E-7 - 6E-7 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of -8E-7 - 6E-7 1/K | for 0-50°C, DIN ISO 51045-1, DIN ISO 7991 |
Conductividad térmica | 90.0 °C | 1.5 - 1.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1.5 - 1.7 W/(m·K) | DIN 51936, ASTM E 1461-01 |
Temperatura máx. de funcionamiento | 650 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 650 °C | short heating (1h) hom. |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 25.0 °C | 6.5 - 7.8 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 6.5 - 7.8 [-] | DIN 53483 |
Resistividad eléctrica | 250.0 °C | 3.98E+6 - 1.58E+7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.98E+6 - 1.58E+7 Ω·m | DIN 52326 |
350.0 °C | 158489 - 501187 Ω·m Show Supplier Material materials with Resistividad eléctrica of 158489 - 501187 Ω·m | DIN 52326 | |
Tangente de pérdidas | 25.0 °C | 0 - 0.02 [-] Show Supplier Material materials with Tangente de pérdidas of 0 - 0.02 [-] | 1MHz, DIN 53483 |
Acústico
Property | Temperature | Value | Comment |
---|---|---|---|
Velocidad del sonido longitudinal | 20.0 °C | 6300 - 6700 m/s Show Supplier Material materials with Velocidad del sonido longitudinal of 6300 - 6700 m/s | ASTM C-1259 |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 15 - 27 % Show Supplier Material materials with Aluminio of 15 - 27 % | Al₂O₃ (DIN EN 1748-2-1) |
Bario | 0 - 8 % Show Supplier Material materials with Bario of 0 - 8 % | BaO (DIN EN 1748-2-1) |
Calcio | 0 - 8 % Show Supplier Material materials with Calcio of 0 - 8 % | CaO (DIN EN 1748-2-1) |
Circonio | 0 - 5 % Show Supplier Material materials with Circonio of 0 - 5 % | ZrO₂ (DIN EN 1748-2-1) |
Litio | 0 - 5 % Show Supplier Material materials with Litio of 0 - 5 % | Li₂O (DIN EN 1748-2-1) |
Magnesio | 0 - 8 % Show Supplier Material materials with Magnesio of 0 - 8 % | MgO (DIN EN 1748-2-1) |
Otro | 0 - 5 % Show Supplier Material materials with Otro of 0 - 5 % | (DIN EN 1748-2-1) |
Potasio | 0 - 2 % Show Supplier Material materials with Potasio of 0 - 2 % | K₂O (DIN EN 1748-2-1) |
Silicona | 50 - 80 % Show Supplier Material materials with Silicona of 50 - 80 % | SiO₂ (DIN EN 1748-2-1) |
Sodio | 0 - 2 % Show Supplier Material materials with Sodio of 0 - 2 % | Na₂O (DIN EN 1748-2-1) |
Titanio | 0 - 5 % Show Supplier Material materials with Titanio of 0 - 5 % | TiO₂ (DIN EN 1748-2-1) |
Zinc | 0 - 5 % Show Supplier Material materials with Zinc of 0 - 5 % | ZnO (DIN EN 1748-2-1) |
Technological properties
Property | ||
---|---|---|
Application areas | The following applications are simply examples of areas where NEXTREMA® has already been put to use successfully: BBQ applications - NEXTREMA® provides perfect visibility into the grill and can be used to optimize diverse aspects of the barbecue experience; IR applications - NEXTREMA® transforms infrared heaters into eye-catching design features and protects heating elements stylishly; High temperature furnaces - Use NEXTREMA® to line ovens or apply support plates (e.g. in display manufacturing); Household appliances - NEXTREMA® revolutionizes designs for transparent heating elements and heat resistant thin film coatings; Functional design material - NEXTREMA® is a revolutionary material for innovative product and industry design. | |
Compliance | NEXTREMA® materials do not contain any harmful substances according to the European directive 2002/95/EC “Hazardous Substances in electrical and electronically Equipment” and fulfill the terms of RoHS without any concerns. | |
Corrosion properties | The chemical resistance of NEXTREMA® is more extensive than that of most other comparable materials: Acid resistance (DIN 12116) S 1-2; Alkaline resistance (ISO 695) A 1-2; Hydrolytic class (DIN ISO 719) HGB 1. | |
Processing methods | NEXTREMA® is practically process inert. Even under extreme conditions, the material will not have negative interactions with the process environment. There are no interfering process factors such as gas emissions from organic components. |