New Material Options for Industrial Processes: Discover NEXTREMA® Glass-Ceramics

SCHOTT AG

Especially in industrial processes, reliability and material performance are key to smooth production. Technical improvements and optimization are influencing factors for success, and new materials often become a crucial factor in evaluating and developing new ways to achieve permanent enhancement.

From flat-panel displays to infrared saunas, industrial paint drying to soldering machines, patio and gastronomy, several applications require parts that are thermally conductive, robust under high temperatures and/or optically transparent.

The NEXTREMA® line of glass-ceramics from SCHOTT AG is a revolutionary solution that combines all of this and more to offer a new range of materials that are promising to displace several thermal material stalwarts.

NEXTREMA® glass-ceramics

NEXTREMA® has a number of key features that make it particularly attractive:

  1. High thermal shock resistance - ability to withstand rapid heat changes
  2. Broad transmission profile in the infrared - suitable for different IR transmitters
  3. Low thermal conductivity - efficient thermal insulation
  4. Robust surface - smooth, chemically inert and scratch-resistant.


Like all materials, the secret to these remarkable properties lie in its microstructure.

NEXTREMA® is not just a glass, it’s a ‘glass-ceramic’. This means that at a microscopic level, tiny ceramic crystals are sprinkled through the glass matrix creating a structure that is much more resistant to heat.

Traditional soda-lime glasses cannot withstand sudden changes in temperature. This is because the glass expands rapidly with heat causing internal stresses that ultimately shatter the glass from within.

The ceramic infusions in NEXTREMA®, however, not only suppress thermal expansion but also provide high heat conductivity ensuring that these materials can withstand huge changes in temperature. This is quantitatively presented in the figure below which plots the variation in size with temperature. Even up to 750°C, the overall thermal expansion is less than 1%.

Thermal expansion in dependence on the temperature (for selected NEXTREMA types)

Moreover, the transparent NEXTREMA® type provides a high transmission in the infrared part which makes it an excellent conductor of heat. This combination of properties makes it highly suitable for applications such as covers for heating elements and flat-panel display manufacturing.

In addition, the chemical inertness of glass-ceramic gives it a smooth and mechanically stable surface that resists scratches and corrosion.

Currently, NEXTREMA® is available in six varieties based on their optical transmission properties:

  1. NEXTREMA® opaque white
  2. NEXTREMA® translucent bluegrey
  3. NEXTREMA® translucent white
  4. NEXTREMA® transparent
  5. NEXTREMA® opaque grey
  6. NEXTREMA® tinted


These six types of NEXTREMA® glass-ceramics all share high thermal shock resistance and low thermal conductivity.

The video below demonstrates the high thermal shock resistance of three NEXTREMA® types: transparent, opaque and translucent. A sheet of each of these NEXTREMA® glasses is heated in an oven to 800°C. They are then taken from the oven and submerged into cold water. A traditional glass shatters at even lower temperature differences when exposed to such an extreme variation in heat. The NEXTREMA® glasses, however, have no problem withstanding the change.


Some specific applications of NEXTREMA® are discussed in the following sections.

Flat-panel display production

Flat-panel display technologies such as AMOLED - Active Matrix Organic Light Emitting Diode - are today the chief means of producing interactive touchpads for smartphones, laptops, smartwatches, and televisions. Touch-sensitive screens are works of complex and meticulous engineering as shown in the figure below.

AMOLED display schematic

Credit: Wikimedia Commons

The light-emitting layer (green) consists of a large number of pixels formed by organic light-emitting diodes (OLED). The pixels are controlled by a large array of thin-film transistors (orange layer) that supply current in the correct proportion to generate light. In general, there are two transistors per pixel.

The use of transistors and organic light-emitting materials have substantially brought down the cost of displays by moving towards low cost, low power and large sizes. Currently, these devices are directly fabricated on amorphous silicon or polycrystalline silicon over plastic substrates, making these displays flexible.

NEXTREMA® as a carrier plate for AMOLED production

The fabrication process involves several heating/baking steps in an oven that need a reliable carrier plate. And this is where NEXTREMA® steps in.

NEXTREMA® glass-ceramic is an excellent carrier plate material due to its near-zero thermal expansion, high thermal shock resistance and its robustness under the high temperatures required for the AMOLED production process.

The display fabrication process involves several rapid heating and cooling steps. The glass-ceramic matrix of NEXTREMA® endow it with a microstructure that can withstand high temperatures as well as rapid changes in temperature without compromising structural integrity.

In addition, the near-zero thermal expansion ensures that the NEXTREMA® carrier plate does not change its shape during the heating process. This could otherwise result in warping of the display and subsequent losses due to scraping.

NEXTREMA® as insulation within the furnace 

Specific NEXTREMA® types make a very good tiling/cladding material for AMOLED ovens.

The high thermal robustness ensures that the tiling can withstand high temperatures for a sustained duration while the near-zero thermal expansion arrests all shrinking and expansion during the heating process.

Furnaces, in general, are very corrosive environments that host highly active gaseous and ionic species. With its high chemical inertness, NEXTREMA® has no interaction with the atmosphere ensuring its continued stability and usability. Further, the non-porous surface does not accumulate dust and other contaminants making it very easy to clean.

NEXTREMA as a furnace insulation material

NEXTREMA® for industrial infrared heating and drying 

The high transmittance of some NEXTREMA® types in the infrared region makes it a highly effective element in several infrared heating and drying processes such as industrial paint drying, food processing and pressing equipment.

These IR heaters require covers that transmit heat while protecting the heating elements from mechanical impact or environmental particles. The combination of high-temperature resistance and IR transparency makes NEXTREMA® the ideal material to be the cover of IR heating equipment.

Further, the surface is easy to clean given the non-porous smooth texture.

Especially in production surroundings, transparent NEXTREMA® is a suitable alternative to quartz glass solutions.

Infrared heater with NEXTREMAInfrared heater with NEXTREMA

NEXTREMA transmission curve

Detailed information on every NEXTREMA® type can be found here:

Artículo de <a href=/suppliers/scho-schott-ag-nextrema-> SCHOTT AG - NEXTREMA® </a>SCHOTT AG - NEXTREMA®

SCHOTT is a leading international technology group in the areas of specialty glass and glass-ceramics. The company has more than 130 years of outstanding development, materials and technology expertise and offers a broad portfolio of high-quality products and intelligent solutions. SCHOTT is an innovative enabler for many industries, including the home appliance, pharma, electronics, optics, life sciences, automotive and aviation industries. SCHOTT strives to play an important part of everyone’s life and is committed to innovation and sustainable success. The parent company, SCHOTT AG, has its headquarters in Mainz (Germany) and is solely owned by the Carl Zeiss Foundation. As a foundation company, SCHOTT assumes special responsibility for its employees, society and the environment. This is also what the SCHOTT NEXTREMA® brand stands for. With high-performance glass-ceramic, SCHOTT offers a portfolio of materials that opens completely new fields of application for engineers and designers with its exceptional technical properties. As a real multi-talent, NEXTREMA® demonstrates what makes glass-ceramic a ground-breaking and unique solution, particularly in high temperature environments.

Enviar una pregunta a

SCHOTT AG - NEXTREMA®

NEXTREMA® is not just a glass, it's a 'glass-ceramic'. The ceramic infusions in NEXTREMA® suppress thermal expansion and also provide high heat conductivity, ensuring that these materials can withstand huge changes in temperature. Even up to 750°C, the overall thermal expansion is less than 1%.