NEXTREMA® is a unique glass-ceramic material platform. This material combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties like an attractive bending strength of 100 - 165 MPa for materials with a thickness of around 4 mm. With a thermal resistance of up to 950 °C, depending on the material type, combined with a thermal shock resistance of 600 - 820 °C, it ensures a reliable material performance even under extreme temperature conditions. Our six unique glass-ceramic types combined with the wide range of sizes and thicknesses varying from 2 mm to 6 mm (> 6 mm on request) will open up new possibilities in product design and performance. The unique transmission spectra provide new ideas for combining innovative infrared heating functionalities with attractive lighting effects. The versatility of this material will surely impress you. In addition, NEXTREMA® opaque grey (712-8) offers the highest maximum temperature resistance of up to 950 °C (1,742 °F) and the highest thermal insulation properties of all NEXTREMA® types due to lowest overall transmission in IR range.

Los datos sobre este material han sido proporcionados por SCHOTT AG.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Densidad

20.0 °C

2.5 - 2.6 g/cm³

Show Supplier Material materials with Densidad of 2.5 - 2.6 g/cm³

approx.

Porosidad

0 %

Show Supplier Material materials with Porosidad of 0 %

approx., ISO 9385

Medidas

PropertyValue

Ancho

900 - 1100 mm

Show Supplier Material materials with Ancho of 900 - 1100 mm

Espesor

3 - 6 mm

Show Supplier Material materials with Espesor of 3 - 6 mm

Longitud

1600 - 1954 mm

Show Supplier Material materials with Longitud of 1600 - 1954 mm

Dimensions

Flat cut-to-size panels and bent panels are also available. Formats of flat cut-to-size panels and bent panels on request.

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

20.0 °C

0.25 - 0.26 [-]

Show Supplier Material materials with Coeficiente de Poisson of 0.25 - 0.26 [-]

approx., ASTM C-1259

Dureza Knoop HK2

20.0 °C

570 - 600 [-]

Show Supplier Material materials with Dureza Knoop HK2 of 570 - 600 [-]

approx., ISO 9385 (HK 0.1/20)

Módulo elástico

20.0 °C

84 - 95 GPa

Show Supplier Material materials with Módulo elástico of 84 - 95 GPa

approx., ASTM C-1259

Resistencia a la flexión

20.0 °C

100 - 165 MPa

Show Supplier Material materials with Resistencia a la flexión of 100 - 165 MPa

approx., DIN EN 1288, Part 5, R45

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

800 - 850 J/(kg·K)

Show Supplier Material materials with Calor específico of 800 - 850 J/(kg·K)

for 20-100°C

Coeficiente de dilatación térmica

50.0 °C

-8E-7 - 6E-7 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of -8E-7 - 6E-7 1/K

for 0-50°C, DIN ISO 51045-1, DIN ISO 7991

Conductividad térmica

90.0 °C

1.5 - 1.7 W/(m·K)

Show Supplier Material materials with Conductividad térmica of 1.5 - 1.7 W/(m·K)

DIN 51936, ASTM E 1461-01

Temperatura máx. de funcionamiento

950 °C

Show Supplier Material materials with Temperatura máx. de funcionamiento of 950 °C

short heating (1h) hom.

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica, 1 MHz

25.0 °C

6.5 - 7.8 [-]

Show Supplier Material materials with Constante dieléctrica, 1 MHz of 6.5 - 7.8 [-]

DIN 53483

Resistividad eléctrica

250.0 °C

3.98E+6 - 1.58E+7 Ω·m

Show Supplier Material materials with Resistividad eléctrica of 3.98E+6 - 1.58E+7 Ω·m

DIN 52326

350.0 °C

158489 - 501187 Ω·m

Show Supplier Material materials with Resistividad eléctrica of 158489 - 501187 Ω·m

DIN 52326

Tangente de pérdidas

25.0 °C

0 - 0.02 [-]

Show Supplier Material materials with Tangente de pérdidas of 0 - 0.02 [-]

1MHz, DIN 53483

Acústico

PropertyTemperatureValueComment

Velocidad del sonido longitudinal

20.0 °C

6300 - 6700 m/s

Show Supplier Material materials with Velocidad del sonido longitudinal of 6300 - 6700 m/s

ASTM C-1259

Chemical properties

PropertyValueComment

Aluminio

15 - 27 %

Show Supplier Material materials with Aluminio of 15 - 27 %

Al₂O₃ (DIN EN 1748-2-1)

Bario

0 - 8 %

Show Supplier Material materials with Bario of 0 - 8 %

BaO (DIN EN 1748-2-1)

Calcio

0 - 8 %

Show Supplier Material materials with Calcio of 0 - 8 %

CaO (DIN EN 1748-2-1)

Circonio

0 - 5 %

Show Supplier Material materials with Circonio of 0 - 5 %

ZrO₂ (DIN EN 1748-2-1)

Litio

0 - 5 %

Show Supplier Material materials with Litio of 0 - 5 %

Li₂O (DIN EN 1748-2-1)

Magnesio

0 - 8 %

Show Supplier Material materials with Magnesio of 0 - 8 %

MgO (DIN EN 1748-2-1)

Otro

0 - 5 %

Show Supplier Material materials with Otro of 0 - 5 %

(DIN EN 1748-2-1)

Potasio

0 - 2 %

Show Supplier Material materials with Potasio of 0 - 2 %

K₂O (DIN EN 1748-2-1)

Silicona

50 - 80 %

Show Supplier Material materials with Silicona of 50 - 80 %

SiO₂ (DIN EN 1748-2-1)

Sodio

0 - 2 %

Show Supplier Material materials with Sodio of 0 - 2 %

Na₂O (DIN EN 1748-2-1)

Titanio

0 - 5 %

Show Supplier Material materials with Titanio of 0 - 5 %

TiO₂ (DIN EN 1748-2-1)

Zinc

0 - 5 %

Show Supplier Material materials with Zinc of 0 - 5 %

ZnO (DIN EN 1748-2-1)

Technological properties

Property
Application areas

The following applications are simply examples of areas where NEXTREMA® has already been put to use successfully: BBQ applications - NEXTREMA® provides perfect visibility into the grill and can be used to optimize diverse aspects of the barbecue experience; IR applications - NEXTREMA® transforms infrared heaters into eye-catching design features and protects heating elements stylishly; High temperature furnaces - Use NEXTREMA® to line ovens or apply support plates (e.g. in display manufacturing); Household appliances - NEXTREMA® revolutionizes designs for transparent heating elements and heat resistant thin film coatings; Functional design material - NEXTREMA® is a revolutionary material for innovative product and industry design.

Compliance

NEXTREMA® materials do not contain any harmful substances according to the European directive 2002/95/EC “Hazardous Substances in electrical and electronically Equipment” and fulfill the terms of RoHS without any concerns.

Corrosion properties

The chemical resistance of NEXTREMA® is more extensive than that of most other comparable materials: Acid resistance (DIN 12116) S 1-2; Alkaline resistance (ISO 695) A 1-2; Hydrolytic class (DIN ISO 719) HGB 1.

Processing methods

NEXTREMA® is practically process inert. Even under extreme conditions, the material will not have negative interactions with the process environment. There are no interfering process factors such as gas emissions from organic components.