General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 145 [-] Show Supplier Material materials with Dureza Vickers of 145 [-] | Minimum |
Módulo elástico | 23.0 °C | 200 GPa Show Supplier Material materials with Módulo elástico of 200 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 9 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9 MPa·√m | |
Resistencia a la flexión | 23.0 °C | 950 MPa Show Supplier Material materials with Resistencia a la flexión of 950 MPa | Minimum |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 400.0 °C | 9.6E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9.6E-6 1/K | Mean value between 20°C and the mentioned temperature, for Zirconium ceramic structural parts |
Conductividad térmica | 23.0 °C | 3 W/(m·K) Show Supplier Material materials with Conductividad térmica of 3 W/(m·K) | Minimum |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Low doping requirement industries:magnetic material,piezoelectric ceramics and dielectric ceramics. Pollution prevention industries:medicine industry,food industry and cosmetic industry. Abrasion and corrosion resistant industries: Coatings,textiles industry,color industry,prinding , dyeing industry, ceramic ink and pesticide industry. Different ceramic material industries:electronic ceramics,refractory ceramics and structural ceramics. |