General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 38 % Show Supplier Material materials with Elongación of 38 % |
Límite elástico | 23.0 °C | 210 MPa Show Supplier Material materials with Límite elástico of 210 MPa |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa |
Resistencia a la tracción | 23.0 °C | 270 - 370 MPa Show Supplier Material materials with Resistencia a la tracción of 270 - 370 MPa |
Chemical properties