General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 17 % Show Supplier Material materials with Elongación of 17 % |
Límite elástico | 23.0 °C | 235 - 245 MPa Show Supplier Material materials with Límite elástico of 235 - 245 MPa |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa |
Resistencia a la tracción | 23.0 °C | 400 - 510 MPa Show Supplier Material materials with Resistencia a la tracción of 400 - 510 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % |
Carbono | 0.21 % Show Supplier Material materials with Carbono of 0.21 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 1.4 % Show Supplier Material materials with Manganeso of 1.4 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |