General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 32 % Show Supplier Material materials with Elongación of 32 % |
Límite elástico | 23.0 °C | 275 - 390 MPa Show Supplier Material materials with Límite elástico of 275 - 390 MPa |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa |
Resistencia a la tracción | 23.0 °C | 275 - 410 MPa Show Supplier Material materials with Resistencia a la tracción of 275 - 410 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Supplier Material materials with Azufre of 0.05 % |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 0.3 - 0.5 % Show Supplier Material materials with Manganeso of 0.3 - 0.5 % |