General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % |
Límite elástico | 23.0 °C | 345 MPa Show Supplier Material materials with Límite elástico of 345 MPa |
Resistencia a la tracción | 23.0 °C | 760 MPa Show Supplier Material materials with Resistencia a la tracción of 760 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.4 % Show Supplier Material materials with Aluminio of 0.4 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | |
Cromo | 20 - 23 % Show Supplier Material materials with Cromo of 20 - 23 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | |
Hierro | 5 % Show Supplier Material materials with Hierro of 5 % | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | |
Molibdeno | 8 - 10 % Show Supplier Material materials with Molibdeno of 8 - 10 % | |
Niobio | 3.15 - 4.15 % Show Supplier Material materials with Niobio of 3.15 - 4.15 % | plus Hydrogen |
Níquel | 58 % Show Supplier Material materials with Níquel of 58 % | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | |
Titanio | 0.4 % Show Supplier Material materials with Titanio of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | 1. The organic chemical process parts contain chloride, especially in the use of acid chloride catalyst. 2. Absorption tower, re-heater, gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system. 3. The equipment and parts in the use of acidic gas environments. 4. Sulfur acid cooling |