General
Property | Value | Comment |
---|---|---|
Densidad | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ASTM D792 |
Medidas
Property | Value |
---|---|
Diámetro | 1.75 mm Show Supplier Material materials with Diámetro of 1.75 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 1.7000000000000002 % Show Supplier Material materials with Elongación of 1.7000000000000002 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 89.0 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 89.0 J/m | ASTM D256 |
Módulo elástico | 11.0 GPa Show Supplier Material materials with Módulo elástico of 11.0 GPa | ASTM D638 |
Resistencia a la tracción | 140.0 MPa Show Supplier Material materials with Resistencia a la tracción of 140.0 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 343.0 °C Show Supplier Material materials with Temperatura de fusión of 343.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace Applications, Automotive Applications, Oil/Gas Applications | |
Certifications | Substances used to manufacture the polymer grade used for this filament meets the requirements of Commission Regulation (EU) N°10/2011, which implements the framework regulation EU 1935/2004 as related to plastic materials and articles intended to come into contact with food and its subsequent amendments as well as the GMP requirements for EU 2023/2006. Please feel free to contact the supplier for RoHS Compliance. | |
Color | Black | |
Features | ||
Fillers | 10% Carbon Fiber | |
Other | Test specimen parameters:
Note: Typical properties: these are not to be construed as specifications | |
Processing methods | Fused Filament Fabrication (FFF) Printing conditions for above data table: |