General
Property | Value | Comment |
---|---|---|
Densidad | 1.72 g/cm³ Show Supplier Material materials with Densidad of 1.72 g/cm³ | ASTM D792, ¹ |
Medidas
Property | Value |
---|---|
Diámetro | 2.85 mm Show Supplier Material materials with Diámetro of 2.85 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 50.0 - 250.0 % Show Supplier Material materials with Elongación of 50.0 - 250.0 % | ASTM D638, ² |
Elongation at yield | 10.0 % Show Supplier Material materials with Elongation at yield of 10.0 % | ASTM D638, ² |
Límite elástico | 30.0 MPa Show Supplier Material materials with Límite elástico of 30.0 MPa | ASTM D638, ² |
Módulo elástico | 0.8 GPa Show Supplier Material materials with Módulo elástico of 0.8 GPa | ASTM D638, ² |
Resistencia a la tracción | 25.0 MPa Show Supplier Material materials with Resistencia a la tracción of 25.0 MPa | ASTM D638 |
Resistencia al choque, ensayo Charpy entallado | 6.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.0 kJ/m² |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 148.0 °C Show Supplier Material materials with Temperatura de fusión of 148.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Manufacturing (3D Printing), Industrial applications, Oil/Gas applications, Plumbing applications | |
Certifications | Substances used to manufacture the polymer grade used for this filament meets the requirements of Commission Regulation (EU) N°10/2011, which implements the framework regulation EU 1935/2004 as related to plastic materials and articles intended to come into contact with food and its subsequent amendments as well as the GMP requirements for EU 2023/2006. Please feel free to contact the supplier for RoHS Compliance. | |
Color | White | |
Features | ||
Other | Test specimen parameters:
Note: Typical properties: these are not to be construed as specifications ¹On 3D printed specimens ²On 3D printed specimens, x-direction | |
Processing methods | Fused Filament Fabrication (FFF) Printing conditions for above data table: |