Property | Value |
---|---|
Ancho | 1000 - 2000 mm Show Supplier Material materials with Ancho of 1000 - 2000 mm |
Espesor | 0.5 - 50 mm Show Supplier Material materials with Espesor of 0.5 - 50 mm |
Longitud | 2000 - 6000 mm Show Supplier Material materials with Longitud of 2000 - 6000 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -195.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Dureza Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] |
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % |
Límite elástico Rp 0,2 | 23.0 °C | 200 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 200 MPa |
Resistencia a la tracción | 23.0 °C | 515 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 515 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % |
Cromo | 17.5 - 19.5 % Show Supplier Material materials with Cromo of 17.5 - 19.5 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Níquel | 8 - 10.5 % Show Supplier Material materials with Níquel of 8 - 10.5 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Material AISI 304/ 304L is used in the chemical industry, food industry, pulp and paper industry and nuclear industry. | |
Corrosion properties | The grade is a versatile, general purpose stainless steel with good resistance to atmospheric corrosion, to many organic and inorganic chemicals, to oxidizing acids like nitric acid, caustic solutions at moderate temperatures and to food and beverages | |
Heat Treatment | Solution annealed and quenched in air or water. | |
Welding | Very good |