General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.85 g/cm³ Show Supplier Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 21 % Show Supplier Material materials with Elongación of 21 % |
Límite elástico | 23.0 °C | 345 MPa Show Supplier Material materials with Límite elástico of 345 MPa |
Resistencia a la tracción | 23.0 °C | 485 MPa Show Supplier Material materials with Resistencia a la tracción of 485 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Supplier Material materials with Azufre of 0.05 % |
Carbono | 0.19 % Show Supplier Material materials with Carbono of 0.19 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Manganeso | 0.8 - 1.25 % Show Supplier Material materials with Manganeso of 0.8 - 1.25 % |
Silicona | 0.3 - 0.65 % Show Supplier Material materials with Silicona of 0.3 - 0.65 % |
Technological properties
Property | ||
---|---|---|
Application areas | Structural Anti-Corrosion Building |