General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | maximum, ASTM D570 |
Densidad | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 60 [-] Show Supplier Material materials with Hardness, Rockwell L of 60 [-] | ASTM D785 |
Módulo de flexión | 23.0 °C | 2.16 GPa Show Supplier Material materials with Módulo de flexión of 2.16 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 54.9 MPa Show Supplier Material materials with Resistencia a la flexión of 54.9 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 30.4 MPa Show Supplier Material materials with Resistencia a la tracción of 30.4 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5E-5 - 1E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5E-5 - 1E-4 1/K | ASTM D696 | ||
Heat deflection temperature, 0.45 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ASTM D648 | |||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 107 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 107 °C | ASTM D1525 | |||
Inflamabilidad | HB UL94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 4 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | AUDIO/TV/VTR HOUSING, HOUSEHOLD ITEMS |