Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-20Suministrada por:
Arkema: High Performance PolymersPolyvinylidenefluoride (PVDF)
Kynar Flex® 2850 BlackSuministrada por:
Arkema: High Performance PolymersPolyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-25Suministrada por:
Arkema: High Performance PolymersPolipropileno
Polypropylene Reinforced with 20% Mineral (PP+M20)Suministrada por:
2 proveedores de Matmatch
Polipropileno
Polypropylene Reinforced with 40% Mineral (PP+M40)Suministrada por:
2 proveedores de Matmatch
Polietileno de alta densidad (PEAD)
High Density Polyethylene (HDPE)Suministrada por:
1 proveedor Matmatch
Polipropileno
Polypropylene Reinforced with 20% Talcum (PP+T20)Suministrada por:
1 proveedor Matmatch