Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-20Suministrada por:
Arkema: High Performance PolymersPolioximetileno (POM)
Delrin® 100P NC010Policarbonato (PC)
LEXAN™ Resin 153RPolioximetileno (POM)
Delrin® 100PE BK602Policarbonato (PC)
LEXAN™ Resin PK2870Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-25Suministrada por:
Arkema: High Performance PolymersPolioximetileno (POM)
Delrin® FG100P NC010Polioximetileno (POM)
Delrin® 100AL NC010Polioximetileno (POM)
Delrin® 127UVE NC010