UGI® 4029

Want to keep this datasheet? Save it now in your required format

Description

A screw machining grade, UGI® 4029 is a martensitic steel whose machinability is improved by the addition of sulphur. Recommended for machined parts with high mechanical properties, it will be used in relatively unaggressive environments (oils, greases, cold detergents, etc.).

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por Ugitech SA.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Chemical properties

PropertyValue

Azufre

0.2 %

Show Supplier Material materials with Azufre of 0.2 %

Carbono

0.28 %

Show Supplier Material materials with Carbono of 0.28 %

Cromo

12.8 %

Show Supplier Material materials with Cromo of 12.8 %

Technological properties

Property
Application areas

Mechanical engineering, transport, food and food processing industry, defence, oil and petrochemicals industry, electronic equipment. Machined parts, screw machining.

Corrosion properties

Corrosion resistance is adversely affected by a high sulphur content compared with martensitic stainless steels with 13% Cr (such as 4021), particularly in environments conducive to pitting or crevice corrosion.

Heat Treatment

Tempering curves on the rigth side of the material page.

Tempering temperature: Indicative mechanical properties after quenching in oil at 950°C and tempering for 2 hours.

Other

Available products:


ProductShapeFinishToleranceDimensions



Bar
RoundRolled and descaled bars12 to 1322 to 15 mm
RoundTurned and polished9 to 1122 to 115 mm
RoundDrawn bar8 to 93 to 55 mm
RoundGround bar6 to 93 to 80 mm
HexagonalDrawn bar113 to 55 mm
Wire rodRoundPickled5.0 to 32 mm
Drawn wireRound16.0 to 1.0 mm


Other products: contact the supplier