General
Property | Value |
---|---|
Densidad | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Value |
---|---|
Elongación | 31.0 - 52.0 % Show Supplier Material materials with Elongación of 31.0 - 52.0 % |
Estricción | 66.0 - 70.0 % Show Supplier Material materials with Estricción of 66.0 - 70.0 % |
Módulo elástico | 200 GPa Show Supplier Material materials with Módulo elástico of 200 GPa |
Resistencia a la tracción | 620.0 - 760.0 MPa Show Supplier Material materials with Resistencia a la tracción of 620.0 - 760.0 MPa |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 0.0000168 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0000168 1/K | 20 to 200°C |
Conductividad térmica | 15 W/(m·K) Show Supplier Material materials with Conductividad térmica of 15 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 7.4e-07 Ω·m Show Supplier Material materials with Resistividad eléctrica of 7.4e-07 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 - 0.03 % Show Supplier Material materials with Azufre of 0.015 - 0.03 % | |
Carbono | 0.05 Show Supplier Material materials with Carbono of 0.05 | max. |
Cromo | 16.5 - 18.5 % Show Supplier Material materials with Cromo of 16.5 - 18.5 % | |
Fósforo | 0.045 Show Supplier Material materials with Fósforo of 0.045 | max. |
Manganeso | 2.0 Show Supplier Material materials with Manganeso of 2.0 | max. |
Molibdeno | 2.0 - 2.5 % Show Supplier Material materials with Molibdeno of 2.0 - 2.5 % | |
Níquel | 10.5 - 11.5 % Show Supplier Material materials with Níquel of 10.5 - 11.5 % | |
Silicona | 1.0 Show Supplier Material materials with Silicona of 1.0 | max. |
Titanio | 0.7000000000000001 Show Supplier Material materials with Titanio of 0.7000000000000001 | max., min: 5xC |
Technological properties
Property | ||
---|---|---|
Corrosion properties | UGIMA® 4571 has excellent ability to withstand corrosion. The table below illustrates a performance scale (with three levels: good/average/excellent) in different environments: | |
General machinability | UGIMA® 4571 offers improved machining performance as a result of the optimization of the inclusion population. This expands the range of cutting conditions suited to the production of machined parts. The productivity gains brought by this new grade are derived from extended tool life, good chip breakability and good surface finish. | |
Heat Treatment | The annealing treatment that gives UGIMA® 4571 its lowest properties includes heating to 1020°C - 1120°C, followed by rapid air or water cooling. | |
Hot forming | Forging: | |
Other | Available products: Do not hesitate to contact the supplier for further information | |
Welding | UGIMA® 4571 can be MIG or TIG welded, with or without filler material, using laser or resistance welding techniques. When using filler wire, we recommend using ER318 (Nb stabilised). For cold applications, ER316LSi wire can also be used. To minimize thermal cracking problems, tight control over welding parameters is required. To do this, always ensure when using arc welding that the linear welding power is limited. |