General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.57 g/cm³ Show Material materials with Densidad of 8.57 g/cm³ | Typical for Niobium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.4 [-] Show Material materials with Coeficiente de Poisson of 0.4 [-] | Typical for Niobium |
Dureza Brinell | 20.0 °C | 135 - 150 [-] Show Material materials with Dureza Brinell of 135 - 150 [-] | |
Módulo de cizallamiento | 23.0 °C | 38 GPa Show Material materials with Módulo de cizallamiento of 38 GPa | Typical for Niobium |
Módulo elástico | 23.0 °C | 104 GPa Show Material materials with Módulo elástico of 104 GPa | Typical for Niobium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 201 - 272 J/(kg·K) Show Material materials with Calor específico of 201 - 272 J/(kg·K) | Typical for Niobium |
Coeficiente de dilatación térmica | 23.0 °C | 6.8E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 6.8E-6 - 1.4E-5 1/K | Typical for Niobium |
Conductividad térmica | 23.0 °C | 53 - 54 W/(m·K) Show Material materials with Conductividad térmica of 53 - 54 W/(m·K) | Typical for Niobium |
Temperatura de fusión | 2468 °C Show Material materials with Temperatura de fusión of 2468 °C | Typical for Niobium |
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Circonio | 0.8 - 1.2 % Show Material materials with Circonio of 0.8 - 1.2 % |
Hafmio | 0.02 % Show Material materials with Hafmio of 0.02 % |
Hidrógeno | 1.5E-3 % Show Material materials with Hidrógeno of 1.5E-3 % |
Hierro | 0.01 % Show Material materials with Hierro of 0.01 % |
Molibdeno | 0.05 % Show Material materials with Molibdeno of 0.05 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Oxígeno | 0.03 % Show Material materials with Oxígeno of 0.03 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Tántalo | 0.5 % Show Material materials with Tántalo of 0.5 % |
Wolframio | 0.05 % Show Material materials with Wolframio of 0.05 % |