General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.57 g/cm³ Show Material materials with Densidad of 8.57 g/cm³ | Typical for Niobium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.4 [-] Show Material materials with Coeficiente de Poisson of 0.4 [-] | Typical for Niobium |
Elongation A25 | 20.0 °C | 20 % Show Material materials with Elongation A25 of 20 % | |
1100.0 °C | 20 % Show Material materials with Elongation A25 of 20 % | ||
Límite elástico Rp 0,2 | 20.0 °C | 260 - 275 MPa Show Material materials with Límite elástico Rp 0,2 of 260 - 275 MPa | |
1100.0 °C | 110 MPa Show Material materials with Límite elástico Rp 0,2 of 110 MPa | ||
Módulo de cizallamiento | 23.0 °C | 38 GPa Show Material materials with Módulo de cizallamiento of 38 GPa | Typical for Niobium |
Módulo elástico | 23.0 °C | 104 GPa Show Material materials with Módulo elástico of 104 GPa | Typical for Niobium |
Resistencia a la tracción | 20.0 °C | 370 - 385 MPa Show Material materials with Resistencia a la tracción of 370 - 385 MPa | |
1100.0 °C | 145 MPa Show Material materials with Resistencia a la tracción of 145 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 201 - 272 J/(kg·K) Show Material materials with Calor específico of 201 - 272 J/(kg·K) | Typical for Niobium |
Coeficiente de dilatación térmica | 23.0 °C | 6.8E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 6.8E-6 - 1.4E-5 1/K | Typical for Niobium |
Conductividad térmica | 23.0 °C | 53 - 54 W/(m·K) Show Material materials with Conductividad térmica of 53 - 54 W/(m·K) | Typical for Niobium |
Temperatura de fusión | 2468 °C Show Material materials with Temperatura de fusión of 2468 °C | Typical for Niobium |
Chemical properties
Property | Value |
---|---|
Carbono | 0.015 % Show Material materials with Carbono of 0.015 % |
Circonio | 0.7 % Show Material materials with Circonio of 0.7 % |
Hafmio | 9 - 11 % Show Material materials with Hafmio of 9 - 11 % |
Hidrógeno | 1.5E-3 % Show Material materials with Hidrógeno of 1.5E-3 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Oxígeno | 0.03 % Show Material materials with Oxígeno of 0.03 % |
Titanio | 0.7 - 1.3 % Show Material materials with Titanio of 0.7 - 1.3 % |
Tántalo | 0.5 % Show Material materials with Tántalo of 0.5 % |
Wolframio | 0.5 % Show Material materials with Wolframio of 0.5 % |