DIN 1725-1 Grade 3.0505 H22

Want to keep this datasheet? Save it now in your required format

Description

The alloy AlMn0,5Mg0,5 is special one for the packing planned alloy. The alloy belongs to the nature-hard aluminum materials. A strength increase can only occur by cold forming. It is very well warm and cold formable and is very well suitable to the deep-drawing (no lappet formation). Because of the good Erichsen index and the relatively high strength (F 24), it finds in addition in architecture use. Standardised is this alloy as sheet metal or strip with a thickness of max. 0,35 mm (DIN 1788). Application: In the packing for menu bowls, light container, bottle caps, doses dose covers as well as in architecture as profile boards for roofs and wall linings and for shutters and suspended covers. For heat exchangers and flexible pipes.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM,AluKey.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueConditionRelated StandardsShape

Densidad

2.71 g/cm³

Show Material materials with Densidad of 2.71 g/cm³

H22

EN 573-3, EN 485

2.72 g/cm³

Show Material materials with Densidad of 2.72 g/cm³

H22

EN 573-3, EN 485

20.0 °C

2.71 g/cm³

Show Material materials with Densidad of 2.71 g/cm³

H22

DIN 1725-1, EN 573-3, EN 573-4

Flat

Mecánica

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coeficiente de Poisson

0.33 [-]

Show Material materials with Coeficiente de Poisson of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Dureza Brinell

41.0 [-]

Show Material materials with Dureza Brinell of 41.0 [-]

H22

EN 573-3, EN 485

Módulo de cizallamiento

25.0 - 26.0 GPa

Show Material materials with Módulo de cizallamiento of 25.0 - 26.0 GPa

Typical for Wrought 3000 Series Aluminium

Módulo elástico

69.0 GPa

Show Material materials with Módulo elástico of 69.0 GPa

H22

EN 573-3, EN 485

70.0 GPa

Show Material materials with Módulo elástico of 70.0 GPa

H22

EN 573-3, EN 485

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Resistencia a la tracción

130.0 - 180.0 MPa

Show Material materials with Resistencia a la tracción of 130.0 - 180.0 MPa

H22

EN 573-3, EN 485

20.0 °C

160.0 - 190.0 MPa

Show Material materials with Resistencia a la tracción of 160.0 - 190.0 MPa

H22

DIN 1725-1, EN 573-3, EN 573-4

Flat

Aplicaciones térmicas

PropertyTemperatureValueConditionRelated StandardsShapeComment

Calor específico

893.0 - 920.0 J/(kg·K)

Show Material materials with Calor específico of 893.0 - 920.0 J/(kg·K)

Typical for Wrought 3000 Series Aluminium

Coeficiente de dilatación térmica

20 °C

2.36e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K

H22

EN 573-3, EN 485

100 °C

2.36e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K

H22

EN 573-3, EN 485

Conductividad térmica

160.0 - 190.0 W/(m·K)

Show Material materials with Conductividad térmica of 160.0 - 190.0 W/(m·K)

H22

EN 573-3, EN 485

172 W/(m·K)

Show Material materials with Conductividad térmica of 172 W/(m·K)

H22

EN 573-3, EN 485

20.0 °C

180.0 - 190.0 W/(m·K)

Show Material materials with Conductividad térmica of 180.0 - 190.0 W/(m·K)

H22

DIN 1725-1, EN 573-3, EN 573-4

Flat

Temperatura de fusión

635.0 - 655.0 °C

Show Material materials with Temperatura de fusión of 635.0 - 655.0 °C

H22

EN 573-3, EN 485

640.0 - 655.0 °C

Show Material materials with Temperatura de fusión of 640.0 - 655.0 °C

H22

EN 573-3, EN 485

Eléctrico

PropertyTemperatureValueConditionRelated StandardsShape

Conductividad eléctrica

23000000.0 - 26000000.0 S/m

Show Material materials with Conductividad eléctrica of 23000000.0 - 26000000.0 S/m

H22

EN 573-3, EN 485

26000000.0 S/m

Show Material materials with Conductividad eléctrica of 26000000.0 S/m

H22

EN 573-3, EN 485

20.0 °C

25000000.0 - 27000000.0 S/m

Show Material materials with Conductividad eléctrica of 25000000.0 - 27000000.0 S/m

H22

DIN 1725-1, EN 573-3, EN 573-4

Flat

Resistividad eléctrica

3.85e-08 Ω·m

Show Material materials with Resistividad eléctrica of 3.85e-08 Ω·m

H22

EN 573-3, EN 485

3.85e-08 - 4.35e-08 Ω·m

Show Material materials with Resistividad eléctrica of 3.85e-08 - 4.35e-08 Ω·m

H22

EN 573-3, EN 485

Chemical properties

PropertyValueConditionRelated StandardsShape

Cobre

0.3 %

Show Material materials with Cobre of 0.3 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Cromo

0.2 %

Show Material materials with Cromo of 0.2 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Hierro

0.7 %

Show Material materials with Hierro of 0.7 %

H22

DIN 1725-1, EN 573-3, EN 573-4

Flat

0.70 %

Show Material materials with Hierro of 0.70 %

H22

EN 573-3, EN 485

Magnesio

0.2 - 0.8 %

Show Material materials with Magnesio of 0.2 - 0.8 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Manganeso

0.3 - 0.8 %

Show Material materials with Manganeso of 0.3 - 0.8 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Silicona

0.6 %

Show Material materials with Silicona of 0.6 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Titanio

0.1 %

Show Material materials with Titanio of 0.1 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Zinc

0.4 %

Show Material materials with Zinc of 0.4 %

H22

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Technological properties

Property
Workability

Good workability.