Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | H14 | EN 573-3, EN 485, EN 541, EN 683 | ||
20.0 °C | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Dureza Brinell | 41.0 [-] Show Material materials with Dureza Brinell of 41.0 [-] | H14 | EN 573-3, EN 485 | |||
20.0 °C | 40.0 [-] Show Material materials with Dureza Brinell of 40.0 [-] | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Elongación | 1.0 % Show Material materials with Elongación of 1.0 % | H14 | EN 573-3, EN 683 | A50 | ||
2.0 % Show Material materials with Elongación of 2.0 % | H14 | EN 573-3, EN 485, EN 541 | A50 | |||
3.0 % Show Material materials with Elongación of 3.0 % | H14 | EN 573-3, EN 485 | A50 | |||
4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3, EN 485 | A50 | |||
5.0 % Show Material materials with Elongación of 5.0 % | H14 | EN 573-3, EN 485 | A50 | |||
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H14 | EN 573-3, EN 485, EN 541, EN 683 | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Resistencia a la tracción | 120.0 - 170.0 MPa Show Material materials with Resistencia a la tracción of 120.0 - 170.0 MPa | H14 | EN 573-3, EN 683 | |||
125.0 - 165.0 MPa Show Material materials with Resistencia a la tracción of 125.0 - 165.0 MPa | H14 | EN 573-3, EN 485, EN 541 | ||||
20.0 °C | 130.0 - 170.0 MPa Show Material materials with Resistencia a la tracción of 130.0 - 170.0 MPa | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | H14 | EN 573-3, EN 485, EN 541, EN 683 | ||
100 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | H14 | EN 573-3, EN 485, EN 541, EN 683 | |||
Conductividad térmica | 20.0 °C | 210.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 210.0 - 220.0 W/(m·K) | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat | |
Temperatura de fusión | 640.0 - 655.0 °C Show Material materials with Temperatura de fusión of 640.0 - 655.0 °C | H14 | EN 573-3, EN 485, EN 541, EN 683 |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 34000000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 34000000.0 - 35000000.0 S/m | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Resistividad eléctrica | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.86e-08 - 2.94e-08 Ω·m | H14 | EN 573-3, EN 485, EN 541, EN 683 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | H14 | EN 573-3, EN 485, EN 541, EN 683 | |
Hierro | 0.5 - 1.0 % Show Material materials with Hierro of 0.5 - 1.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Magnesio | 0.1 % Show Material materials with Magnesio of 0.1 % | H14 | EN 573-3, EN 485, EN 541, EN 683 | |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |
Titanio | 0.05 Show Material materials with Titanio of 0.05 | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H14 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 683 | Flat |