General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | ||
20.0 °C | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 100.0 MPa Show Material materials with Bending Fatigue Strength of 100.0 MPa | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | |||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Dureza Brinell | 44.0 [-] Show Material materials with Dureza Brinell of 44.0 [-] | O | EN 573-3, EN 485 | |||
20.0 °C | 40.0 [-] Show Material materials with Dureza Brinell of 40.0 [-] | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube, Wire | ||
20.0 °C | 45.0 [-] Show Material materials with Dureza Brinell of 45.0 [-] | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
Elongación | 13.0 % Show Material materials with Elongación of 13.0 % | O | EN 573-3, EN 1396, EN 485 | A50 | ||
14.0 % Show Material materials with Elongación of 14.0 % | O | EN 573-3, EN 1396, EN 485 | A50 | |||
15.0 % Show Material materials with Elongación of 15.0 % | O | EN 573-3, EN 1301 | ||||
15.0 % Show Material materials with Elongación of 15.0 % | O | EN 573-3, EN 754, EN 755 | A50 | |||
16.0 % Show Material materials with Elongación of 16.0 % | O | EN 573-3, EN 1396, EN 485 | A50 | |||
17.0 % Show Material materials with Elongación of 17.0 % | O | EN 573-3, EN 754, EN 755 | A100 | |||
18.0 % Show Material materials with Elongación of 18.0 % | O | EN 573-3, EN 485 | A100 | |||
18.0 % Show Material materials with Elongación of 18.0 % | O | EN 573-3, EN 485 | A50 | |||
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Wire | A100 | |
20.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Wire | A10 | |
20.0 °C | 15.0 % Show Material materials with Elongación of 15.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | A10 | |
20.0 °C | 17.0 % Show Material materials with Elongación of 17.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | A10 | |
20.0 °C | 17.0 % Show Material materials with Elongación of 17.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | ||
20.0 °C | 20.0 % Show Material materials with Elongación of 20.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
Módulo de cizallamiento | 26.3 GPa Show Material materials with Módulo de cizallamiento of 26.3 GPa | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | |||
20.0 °C | 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.5 GPa | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire | ||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | |||
20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 150.0 - 200.0 MPa Show Material materials with Resistencia a la tracción of 150.0 - 200.0 MPa | O | EN 573-3, EN 754 | |||
160.0 - 200.0 MPa Show Material materials with Resistencia a la tracción of 160.0 - 200.0 MPa | O | EN 573-3, EN 1396, EN 485 | ||||
160.0 - 220.0 MPa Show Material materials with Resistencia a la tracción of 160.0 - 220.0 MPa | O | EN 573-3, EN 755 | ||||
215.0 MPa Show Material materials with Resistencia a la tracción of 215.0 MPa | O | EN 573-3, EN 1301 | ||||
20.0 °C | 150.0 MPa Show Material materials with Resistencia a la tracción of 150.0 MPa | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube, Wire | ||
20.0 °C | 155.0 - 200.0 MPa Show Material materials with Resistencia a la tracción of 155.0 - 200.0 MPa | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
Ángulo de flexión a 180° | 0.5 °/t Show Material materials with Ángulo de flexión a 180° of 0.5 °/t | O | EN 573-3, EN 485 | |||
Ángulo de flexión a 90° | 0.5 °/t Show Material materials with Ángulo de flexión a 90° of 0.5 °/t | O | EN 573-3, EN 485 | |||
1.0 °/t Show Material materials with Ángulo de flexión a 90° of 1.0 °/t | O | EN 573-3, EN 485 | ||||
2.0 °/t Show Material materials with Ángulo de flexión a 90° of 2.0 °/t | O | EN 573-3, EN 485 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire | |
Coeficiente de dilatación térmica | 20 °C | 2.3699999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3699999999999997e-05 1/K | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | ||
100 °C | 2.3699999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3699999999999997e-05 1/K | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | |||
Conductividad térmica | 140.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 - 160.0 W/(m·K) | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | |||
20.0 °C | 167.0 W/(m·K) Show Material materials with Conductividad térmica of 167.0 W/(m·K) | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire | ||
Temperatura de fusión | 610.0 - 650.0 °C Show Material materials with Temperatura de fusión of 610.0 - 650.0 °C | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | |||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 25000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 25000000.0 - 30000000.0 S/m | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | ||
20.0 °C | 26000000.0 S/m Show Material materials with Conductividad eléctrica of 26000000.0 S/m | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire | |
Resistividad eléctrica | 3.33e-08 - 4e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.33e-08 - 4e-08 Ω·m | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet, Strip, Tube, Wire |
0.50 % Show Material materials with Hierro of 0.50 % | O | EN 573-3, EN 1301, EN 1396, EN 485, EN 754, EN 755 | ||
Magnesio | 1.7 - 2.4 % Show Material materials with Magnesio of 1.7 - 2.4 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Manganeso | 0.1 - 0.5 % Show Material materials with Manganeso of 0.1 - 0.5 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Zinc | 0.15 % Show Material materials with Zinc of 0.15 % | O | DIN 1725-1, EN 573-3, EN 573-4, EN 1301, EN 1396, EN 485, EN 754, EN 755 | Rod, Sheet, Strip, Tube, Wire |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): sufficient / poor, friction soldering: good, soft brazing with flux: sufficient | |
Corrosion properties | Seawater: good, weathering: very good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) good (O) / acceptable (H12) |