General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 60.0 [-] Show Material materials with Dureza Brinell of 60.0 [-] | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
20.0 °C | 72.0 [-] Show Material materials with Dureza Brinell of 72.0 [-] | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Elongación | 20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | A100 |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | A10 | |
Módulo de cizallamiento | 20.0 °C | 26.5 Show Material materials with Módulo de cizallamiento of 26.5 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire | |
Módulo elástico | 20.0 °C | 70.0 Show Material materials with Módulo elástico of 70.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
20.0 °C | 230.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 270.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Resistencia al cizallamiento | 20.0 °C | 130.0 MPa Show Material materials with Resistencia al cizallamiento of 130.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire | |
Coeficiente de dilatación térmica | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 167.0 Show Material materials with Conductividad térmica of 167.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire | |
Temperatura de fusión | 560.0 - 655.0 °C Show Material materials with Temperatura de fusión of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 26000000.0 Show Material materials with Conductividad eléctrica of 26000000.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire | |
Resistividad eléctrica | 3.3e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 Show Material materials with Cobre of 0.15 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Cromo | 0.15 Show Material materials with Cromo of 0.15 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Magnesio | 1.7 - 2.4 % Show Material materials with Magnesio of 1.7 - 2.4 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Manganeso | 0.1 - 0.5 % Show Material materials with Manganeso of 0.1 - 0.5 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Silicona | 0.4 Show Material materials with Silicona of 0.4 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Titanio | 0.15 Show Material materials with Titanio of 0.15 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Zinc | 0.15 Show Material materials with Zinc of 0.15 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat, Wire |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |