General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.77 g/cm³ Show Material materials with Densidad of 2.77 g/cm³ | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 100.0 [-] Show Material materials with Dureza Brinell of 100.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Rod | |
20.0 °C | 100.0 - 105.0 [-] Show Material materials with Dureza Brinell of 100.0 - 105.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Rod | ||
20.0 °C | 105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod | ||
Elongación | 20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Rod | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod | A10 | |
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Sheet | ||
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod | ||
Módulo de cizallamiento | 20.0 °C | 25.0 - 27.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 - 27.0 GPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Módulo elástico | 20.0 °C | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 340.0 MPa Show Material materials with Resistencia a la tracción of 340.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Sheet | |
20.0 °C | 350.0 MPa Show Material materials with Resistencia a la tracción of 350.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 875.0 J/(kg·K) Show Material materials with Calor específico of 875.0 J/(kg·K) | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Coeficiente de dilatación térmica | -50.0 °C | 2.14e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.14e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
100.0 °C | 2.31e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.31e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | ||
200.0 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | ||
300.0 °C | 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | ||
Conductividad térmica | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 160.0 W/(m·K) | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 19000000.0 - 23000000.0 S/m | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Circonio | 0.08 - 0.2 % Show Material materials with Circonio of 0.08 - 0.2 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Cobre | 0.2 Show Material materials with Cobre of 0.2 | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Cromo | 0.1 - 0.35 % Show Material materials with Cromo of 0.1 - 0.35 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Hierro | 0.4 Show Material materials with Hierro of 0.4 | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Magnesio | 1.0 - 1.4 % Show Material materials with Magnesio of 1.0 - 1.4 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Manganeso | 0.05 - 0.5 % Show Material materials with Manganeso of 0.05 - 0.5 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Silicona | 0.35 Show Material materials with Silicona of 0.35 | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Zinc | 4.0 - 5.0 % Show Material materials with Zinc of 4.0 - 5.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |