General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.78 g/cm³ Show Material materials with Densidad of 2.78 g/cm³ | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 100.0 [-] Show Material materials with Dureza Brinell of 100.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | |
20.0 °C | 110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | ||
20.0 °C | 125.0 [-] Show Material materials with Dureza Brinell of 125.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Sheet | ||
20.0 °C | 130.0 [-] Show Material materials with Dureza Brinell of 130.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | ||
20.0 °C | 140.0 [-] Show Material materials with Dureza Brinell of 140.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile | ||
Elongación | 20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | ||
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod | A10 | |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | A10 | |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet | ||
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Tube, Sheet | ||
Módulo de cizallamiento | 20.0 °C | 27.5 GPa Show Material materials with Módulo de cizallamiento of 27.5 GPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube | |
Módulo elástico | 20.0 °C | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 410.0 MPa Show Material materials with Resistencia a la tracción of 410.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | |
20.0 °C | 430.0 MPa Show Material materials with Resistencia a la tracción of 430.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | ||
20.0 °C | 450.0 MPa Show Material materials with Resistencia a la tracción of 450.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet | ||
20.0 °C | 460.0 MPa Show Material materials with Resistencia a la tracción of 460.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Rod | ||
20.0 °C | 470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | ||
20.0 °C | 490.0 MPa Show Material materials with Resistencia a la tracción of 490.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 795.0 - 1050.0 J/(kg·K) Show Material materials with Calor específico of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 160.0 W/(m·K) | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube | |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 19000000.0 - 23000000.0 S/m | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube | |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.5 - 1.0 % Show Material materials with Cobre of 0.5 - 1.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Cromo | 0.1 - 0.3 % Show Material materials with Cromo of 0.1 - 0.3 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Magnesio | 2.6 - 3.7 % Show Material materials with Magnesio of 2.6 - 3.7 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Manganeso | 0.1 - 0.4 % Show Material materials with Manganeso of 0.1 - 0.4 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Silicona | 0.5 Show Material materials with Silicona of 0.5 | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Zinc | 4.3 - 5.2 % Show Material materials with Zinc of 4.3 - 5.2 % | T8 | DIN 1725-1, EN 573-3, EN 573-4 | Profile, Rod, Sheet, Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |