General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 32.0 [-] Show Material materials with Dureza Brinell of 32.0 [-] | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Rod | |
20.0 °C | 32.0 - 48.0 [-] Show Material materials with Dureza Brinell of 32.0 - 48.0 [-] | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Flat | ||
Elongación | 20.0 °C | 1.0 % Show Material materials with Elongación of 1.0 % | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire | A200 |
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire | A100 | |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Rod | A10 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Flat | ||
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Rod | ||
Módulo de cizallamiento | 20.0 °C | 25.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 25.0 - 26.5 GPa | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat | |
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 130.0 - 180.0 MPa Show Material materials with Resistencia a la tracción of 130.0 - 180.0 MPa | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire | |
20.0 °C | 130.0 MPa Show Material materials with Resistencia a la tracción of 130.0 MPa | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Rod | ||
20.0 °C | 130.0 - 170.0 MPa Show Material materials with Resistencia a la tracción of 130.0 - 170.0 MPa | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Flat |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat | |
Coeficiente de dilatación térmica | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 230.0 W/(m·K) Show Material materials with Conductividad térmica of 230.0 W/(m·K) | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat | |
Temperatura de fusión | 645.0 - 660.0 °C Show Material materials with Temperatura de fusión of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 33000000.0 - 38000000.0 S/m Show Material materials with Conductividad eléctrica of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Resistividad eléctrica | 2.7e-08 - 3e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.02 Show Material materials with Cobre of 0.02 | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat |
Hierro | 0.4 Show Material materials with Hierro of 0.4 | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat |
Magnesio | 0.05 Show Material materials with Magnesio of 0.05 | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat |
Silicona | 0.25 Show Material materials with Silicona of 0.25 | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat |
Zinc | 0.05 Show Material materials with Zinc of 0.05 | H18 | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Rod, Flat |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |