General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.67 g/cm³ Show Material materials with Densidad of 2.67 g/cm³ | O | EN 573-3, EN 485 | |
2.67 g/cm³ Show Material materials with Densidad of 2.67 g/cm³ | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Elongación | 18.0 % Show Material materials with Elongación of 18.0 % | O | EN 573-3, EN 485 | |||
18.0 % Show Material materials with Elongación of 18.0 % | O | EN 573-3, EN 485 | A50 | |||
20.0 °C | 18.0 % Show Material materials with Elongación of 18.0 % | O | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 18.0 % Show Material materials with Elongación of 18.0 % | O | EN 573-3 | Flat | Transverse | |
Módulo de cizallamiento | 27.6 GPa Show Material materials with Módulo de cizallamiento of 27.6 GPa | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | ||
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 240.0 - 350.0 MPa Show Material materials with Resistencia a la tracción of 240.0 - 350.0 MPa | O | EN 573-3, EN 485 | |||
20.0 °C | 240.0 - 350.0 MPa Show Material materials with Resistencia a la tracción of 240.0 - 350.0 MPa | O | EN 573-3 | Flat | Transverse | |
Ángulo de flexión a 180° | 1.5 °/t Show Material materials with Ángulo de flexión a 180° of 1.5 °/t | O | EN 573-3, EN 485 | |||
2.0 °/t Show Material materials with Ángulo de flexión a 180° of 2.0 °/t | O | EN 573-3, EN 485 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 879.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | 20-100°C |
Conductividad térmica | 125 W/(m·K) Show Material materials with Conductividad térmica of 125 W/(m·K) | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | ||
Temperatura de fusión | 560.0 - 655.0 °C Show Material materials with Temperatura de fusión of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Conductividad eléctrica | 18000000.0 - 31000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium | |||
Resistividad eléctrica | 5.7e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.7e-08 Ω·m | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % | O | EN 573-3, EN 485 | Flat |
0.15 % Show Material materials with Cobre of 0.15 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | O | EN 573-3, EN 485 | Flat |
0.1 % Show Material materials with Cromo of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % | O | EN 573-3 | Flat |
0.35 % Show Material materials with Hierro of 0.35 % | O | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | |
Magnesio | 3.0 - 4.0 % Show Material materials with Magnesio of 3.0 - 4.0 % | O | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Flat, Coil, Sheet, Plate |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % | O | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Flat, Coil, Sheet, Plate |
Otro | 0.05 - 0.15 % Show Material materials with Otro of 0.05 - 0.15 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | O | EN 573-3, EN 485 | Flat |
0.2 % Show Material materials with Silicona of 0.2 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | O | EN 573-3 | Flat |
0.1 % Show Material materials with Titanio of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate | |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | O | EN 573-3, EN 485 | Flat |
0.25 % Show Material materials with Zinc of 0.25 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent (anodizing quality) | |
Application areas | Vessels: Pressure; Wind energy: Nacelle coverings, rotor hub, stairs; Food can: Body, Lids; Components: Access hatches, Spoilers, General transportation | |
Corrosion properties | Excellent | |
Welding | Good | |
Workability | Good (in O temper) |