Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 140 - 180 W/(m·K) Show Material materials with Conductividad térmica of 140 - 180 W/(m·K) |
Temperatura de fusión | 650 °C Show Material materials with Temperatura de fusión of 650 °C | |
Temperatura máx. de funcionamiento, largo | 150 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 150 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.00E+7 - 2.50E+7 S/m Show Material materials with Conductividad eléctrica of 2.00E+7 - 2.50E+7 S/m |
General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.7 - 2.71 g/cm³ Show Material materials with Densidad of 2.7 - 2.71 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Límite elástico Rp 0,2 | 20.0 °C | 70 - 80 MPa Show Material materials with Límite elástico Rp 0,2 of 70 - 80 MPa |
Módulo elástico | -270.0 °C | 70 GPa Show Material materials with Módulo elástico of 70 GPa |
20.0 °C | 70 GPa Show Material materials with Módulo elástico of 70 GPa | |
50.0 °C | 69 GPa Show Material materials with Módulo elástico of 69 GPa | |
100.0 °C | 68 GPa Show Material materials with Módulo elástico of 68 GPa | |
150.0 °C | 66 GPa Show Material materials with Módulo elástico of 66 GPa | |
200.0 °C | 63 GPa Show Material materials with Módulo elástico of 63 GPa | |
250.0 °C | 57 GPa Show Material materials with Módulo elástico of 57 GPa | |
300.0 °C | 50 GPa Show Material materials with Módulo elástico of 50 GPa | |
Chemical properties
Property | Value |
---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Magnesio | 1.6 - 2.5 % Show Material materials with Magnesio of 1.6 - 2.5 % |
Manganeso | 0.5 - 1.1 % Show Material materials with Manganeso of 0.5 - 1.1 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |