General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.84 g/cm³ Show Material materials with Densidad of 2.75 - 2.84 g/cm³ | Typical for Wrought 2000 Series Aluminium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Elongación | 20.0 °C | 11.0 % Show Material materials with Elongación of 11.0 % | F46 | WL 3.1254-1 | |
100.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | F46 | WL 3.1254-1 | ||
150.0 °C | 30.0 % Show Material materials with Elongación of 30.0 % | F46 | WL 3.1254-1 | ||
200.0 °C | 55.0 % Show Material materials with Elongación of 55.0 % | F46 | WL 3.1254-1 | ||
260.0 °C | 65.0 % Show Material materials with Elongación of 65.0 % | F46 | WL 3.1254-1 | ||
315.0 °C | 70.0 % Show Material materials with Elongación of 70.0 % | F46 | WL 3.1254-1 | ||
370.0 °C | 70.0 % Show Material materials with Elongación of 70.0 % | F46 | WL 3.1254-1 | ||
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | |||
Módulo elástico | 70.0 - 73.0 GPa Show Material materials with Módulo elástico of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Resistencia a la tracción | 20.0 °C | 480.0 MPa Show Material materials with Resistencia a la tracción of 480.0 MPa | F46 | WL 3.1254-1 | |
100.0 °C | 435.0 MPa Show Material materials with Resistencia a la tracción of 435.0 MPa | F46 | WL 3.1254-1 | ||
150.0 °C | 275.0 MPa Show Material materials with Resistencia a la tracción of 275.0 MPa | F46 | WL 3.1254-1 | ||
200.0 °C | 110.0 MPa Show Material materials with Resistencia a la tracción of 110.0 MPa | F46 | WL 3.1254-1 | ||
260.0 °C | 65.0 MPa Show Material materials with Resistencia a la tracción of 65.0 MPa | F46 | WL 3.1254-1 | ||
315.0 °C | 45.0 MPa Show Material materials with Resistencia a la tracción of 45.0 MPa | F46 | WL 3.1254-1 | ||
370.0 °C | 30.0 MPa Show Material materials with Resistencia a la tracción of 30.0 MPa | F46 | WL 3.1254-1 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Conductividad térmica | 112.0 - 251.0 W/(m·K) Show Material materials with Conductividad térmica of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Temperatura de fusión | 500.0 - 650.0 °C Show Material materials with Temperatura de fusión of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 3.9 - 5.0 % Show Material materials with Cobre of 3.9 - 5.0 % | F46 | WL 3.1254-1 |
Cromo | 0.1 Show Material materials with Cromo of 0.1 | F46 | WL 3.1254-1 |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | F46 | WL 3.1254-1 |
Magnesio | 0.2 - 0.8 % Show Material materials with Magnesio of 0.2 - 0.8 % | F46 | WL 3.1254-1 |
Manganeso | 0.4 - 1.2 % Show Material materials with Manganeso of 0.4 - 1.2 % | F46 | WL 3.1254-1 |
Silicona | 0.5 - 1.2 % Show Material materials with Silicona of 0.5 - 1.2 % | F46 | WL 3.1254-1 |
Titanio | 0.15 Show Material materials with Titanio of 0.15 | F46 | WL 3.1254-1 |
Zinc | 0.25 Show Material materials with Zinc of 0.25 | F46 | WL 3.1254-1 |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |