General
Property | Value | Comment |
---|---|---|
Densidad | 2.7 - 2.85 g/cm³ Show Material materials with Densidad of 2.7 - 2.85 g/cm³ | Typical for Wrought 7000 Series Aluminium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Elongación | 20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T73 | WL 3.4144-1 | Wire | |
Módulo de cizallamiento | 26.4 - 27.1 GPa Show Material materials with Módulo de cizallamiento of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 480.0 MPa Show Material materials with Resistencia a la tracción of 480.0 MPa | T73 | WL 3.4144-1 | Wire | |
Resistencia al cizallamiento | 20.0 °C | 280.0 - 320.0 MPa Show Material materials with Resistencia al cizallamiento of 280.0 - 320.0 MPa | T73 | WL 3.4144-1 | Wire |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 100.0 °C | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | T73 | WL 3.4144-1 | Wire | |
Coeficiente de dilatación térmica | 100.0 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T73 | WL 3.4144-1 | Wire | |
200.0 °C | 2.43e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.43e-05 1/K | T73 | WL 3.4144-1 | Wire | ||
300.0 °C | 2.52e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.52e-05 1/K | T73 | WL 3.4144-1 | Wire | ||
Conductividad térmica | 25.0 °C | 157.0 W/(m·K) Show Material materials with Conductividad térmica of 157.0 W/(m·K) | T73 | WL 3.4144-1 | Wire | |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Circonio | 0.08 - 0.15 % Show Material materials with Circonio of 0.08 - 0.15 % | T73 | WL 3.4144-1 | Wire |
Cobre | 2.0 - 2.6 % Show Material materials with Cobre of 2.0 - 2.6 % | T73 | WL 3.4144-1 | Wire |
Cromo | 0.04 Show Material materials with Cromo of 0.04 | T73 | WL 3.4144-1 | Wire |
Hierro | 0.15 Show Material materials with Hierro of 0.15 | T73 | WL 3.4144-1 | Wire |
Magnesio | 1.9 - 2.6 % Show Material materials with Magnesio of 1.9 - 2.6 % | T73 | WL 3.4144-1 | Wire |
Manganeso | 0.1 Show Material materials with Manganeso of 0.1 | T73 | WL 3.4144-1 | Wire |
Silicona | 0.12 Show Material materials with Silicona of 0.12 | T73 | WL 3.4144-1 | Wire |
Titanio | 0.06 Show Material materials with Titanio of 0.06 | T73 | WL 3.4144-1 | Wire |
Zinc | 5.7 - 6.7 % Show Material materials with Zinc of 5.7 - 6.7 % | T73 | WL 3.4144-1 | Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |