General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.82 g/cm³ Show Material materials with Densidad of 2.82 g/cm³ | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Dureza Brinell | 135.0 [-] Show Material materials with Dureza Brinell of 135.0 [-] | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
20.0 °C | 135.0 [-] Show Material materials with Dureza Brinell of 135.0 [-] | T7452 | WL 3.4394 | Forging | ||
Elongación | 9.0 % Show Material materials with Elongación of 9.0 % | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | A50 | |
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | T7452 | WL 3.4394 | Forging | ||
Módulo de cizallamiento | 27.0 GPa Show Material materials with Módulo de cizallamiento of 27.0 GPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Resistencia a la tracción | 480.0 MPa Show Material materials with Resistencia a la tracción of 480.0 MPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
490.0 MPa Show Material materials with Resistencia a la tracción of 490.0 MPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | |||
495.0 MPa Show Material materials with Resistencia a la tracción of 495.0 MPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | |||
20.0 °C | 460.0 MPa Show Material materials with Resistencia a la tracción of 460.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 475.0 MPa Show Material materials with Resistencia a la tracción of 475.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 480.0 MPa Show Material materials with Resistencia a la tracción of 480.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 490.0 MPa Show Material materials with Resistencia a la tracción of 490.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 495.0 MPa Show Material materials with Resistencia a la tracción of 495.0 MPa | T7452 | WL 3.4394 | Forging |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 795.0 - 1050.0 J/(kg·K) Show Material materials with Calor específico of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Coeficiente de dilatación térmica | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Conductividad térmica | 121.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 23000000.0 - 25000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 25000000.0 S/m | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire |
Resistividad eléctrica | 4e-08 - 4.35e-08 Ω·m Show Material materials with Resistividad eléctrica of 4e-08 - 4.35e-08 Ω·m | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Circonio | 0.1 - 0.16 % Show Material materials with Circonio of 0.1 - 0.16 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Cobre | 1.5 - 2.0 % Show Material materials with Cobre of 1.5 - 2.0 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | T7452 | WL 3.4394 | Forging |
0.15 % Show Material materials with Hierro of 0.15 % | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | |
Magnesio | 2.1 - 2.6 % Show Material materials with Magnesio of 2.1 - 2.6 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Níquel | 0.05 % Show Material materials with Níquel of 0.05 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Silicona | 0.12 % Show Material materials with Silicona of 0.12 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Titanio | 0.06 % Show Material materials with Titanio of 0.06 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Zinc | 5.7 - 6.7 % Show Material materials with Zinc of 5.7 - 6.7 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |