General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.85 g/cm³ Show Material materials with Densidad of 2.85 g/cm³ | T4510 | EN 573-3, EN 755 | Rod, Tube | |
20.0 °C | 2.85 g/cm³ Show Material materials with Densidad of 2.85 g/cm³ | T4510 | EN 573-3 | Profile, Rod, Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 95.0 [-] Show Material materials with Dureza Brinell of 95.0 [-] | T4510 | EN 573-3 | Profile, Rod, Tube | |
Elongación | 6.0 % Show Material materials with Elongación of 6.0 % | T4510 | EN 573-3, EN 755 | Rod, Tube | A50 | |
7.0 % Show Material materials with Elongación of 7.0 % | T4510 | EN 573-3, EN 755 | Rod, Tube | A100 | ||
8.0 % Show Material materials with Elongación of 8.0 % | T4510 | EN 573-3, EN 755 | Rod, Tube | A100 | ||
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T4510 | EN 573-3 | Profile, Rod, Tube | A50 | |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T4510 | EN 573-3 | Rod | ||
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T4510 | EN 573-3 | Profile, Tube, Rod | ||
Módulo de cizallamiento | 27.3 GPa Show Material materials with Módulo de cizallamiento of 27.3 GPa | T4510 | EN 573-3, EN 755 | Rod, Tube | ||
Módulo elástico | 72.5 GPa Show Material materials with Módulo elástico of 72.5 GPa | T4510 | EN 573-3, EN 755 | Rod, Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Resistencia a la tracción | 330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | T4510 | EN 573-3, EN 755 | Rod, Tube | ||
340.0 MPa Show Material materials with Resistencia a la tracción of 340.0 MPa | T4510 | EN 573-3, EN 755 | Rod, Tube | |||
370.0 MPa Show Material materials with Resistencia a la tracción of 370.0 MPa | T4510 | EN 573-3, EN 755 | Rod, Tube | |||
20.0 °C | 330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | T4510 | EN 573-3 | Rod | ||
20.0 °C | 340.0 MPa Show Material materials with Resistencia a la tracción of 340.0 MPa | T4510 | EN 573-3 | Rod | ||
20.0 °C | 370.0 MPa Show Material materials with Resistencia a la tracción of 370.0 MPa | T4510 | EN 573-3 | Profile, Tube, Rod |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 860.0 J/(kg·K) Show Material materials with Calor específico of 860.0 J/(kg·K) | T4510 | EN 573-3, EN 755 | Rod, Tube | |
20.0 °C | 860.0 J/(kg·K) Show Material materials with Calor específico of 860.0 J/(kg·K) | T4510 | EN 573-3 | Profile, Rod, Tube | |
Coeficiente de dilatación térmica | 20 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T4510 | EN 573-3, EN 755 | Rod, Tube |
100 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T4510 | EN 573-3, EN 755 | Rod, Tube | |
100.0 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | T4510 | EN 573-3 | Profile, Rod, Tube | |
Conductividad térmica | 130.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 160.0 W/(m·K) | T4510 | EN 573-3, EN 755 | Rod, Tube | |
20.0 °C | 116.0 - 168.0 W/(m·K) Show Material materials with Conductividad térmica of 116.0 - 168.0 W/(m·K) | T4510 | EN 573-3 | Profile, Rod, Tube | |
Temperatura de fusión | 507.0 - 650.0 °C Show Material materials with Temperatura de fusión of 507.0 - 650.0 °C | T4510 | EN 573-3, EN 755 | Rod, Tube |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 18000000.0 - 22000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 22000000.0 S/m | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Resistividad eléctrica | 4.55e-08 - 5.56e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.55e-08 - 5.56e-08 Ω·m | T4510 | EN 573-3, EN 755 | Rod, Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bismuto | 0.2 % Show Material materials with Bismuto of 0.2 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Cobre | 3.3 - 4.6 % Show Material materials with Cobre of 3.3 - 4.6 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % | T4510 | EN 573-3 | Profile, Rod, Tube |
0.80 % Show Material materials with Hierro of 0.80 % | T4510 | EN 573-3, EN 755 | Rod, Tube | |
Magnesio | 0.4 - 1.8 % Show Material materials with Magnesio of 0.4 - 1.8 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Manganeso | 0.5 - 1.0 % Show Material materials with Manganeso of 0.5 - 1.0 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Plomo | 0.8 - 1.5 % Show Material materials with Plomo of 0.8 - 1.5 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Zinc | 0.8 % Show Material materials with Zinc of 0.8 % | T4510 | EN 573-3, EN 755 | Profile, Rod, Tube |
Technological properties
Property | ||
---|---|---|
Anodizing | Protective: poor | |
Brazing | friction soldering: sufficient | |
Corrosion properties | Seawater: poor, weathering: poor | |
Workability | Bending / Spinning (cold): sufficient / -, Deep drawing / upsetting (Condition) - / sufficient |