General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 4000 Series Aluminium | ||
Módulo de cizallamiento | 26.0 GPa Show Material materials with Módulo de cizallamiento of 26.0 GPa | Typical for Wrought 4000 Series Aluminium | ||
Módulo elástico | 79.0 GPa Show Material materials with Módulo elástico of 79.0 GPa | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 864.0 J/(kg·K) Show Material materials with Calor específico of 864.0 J/(kg·K) | Typical for Wrought 4000 Series Aluminium | |||
Coeficiente de dilatación térmica | 20 °C | 1.9399999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9399999999999997e-05 1/K | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 1.9399999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9399999999999997e-05 1/K | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | ||
Conductividad térmica | 138.0 - 155.0 W/(m·K) Show Material materials with Conductividad térmica of 138.0 - 155.0 W/(m·K) | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | ||
Temperatura de fusión | 530.0 - 570.0 °C Show Material materials with Temperatura de fusión of 530.0 - 570.0 °C | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Eléctrico
Property | Value | Related Standards | Shape |
---|---|---|---|
Conductividad eléctrica | 20000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 20000000.0 - 23000000.0 S/m | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Resistividad eléctrica | 4.35e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.35e-08 - 5e-08 Ω·m | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Cobre | 0.5 - 1.3 % Show Material materials with Cobre of 0.5 - 1.3 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Hierro | 1.0 % Show Material materials with Hierro of 1.0 % | EN 573-3 | |
1.00 % Show Material materials with Hierro of 1.00 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
Magnesio | 0.8 - 1.3 % Show Material materials with Magnesio of 0.8 - 1.3 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Níquel | 0.5 - 1.3 % Show Material materials with Níquel of 0.5 - 1.3 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Silicona | 11.0 - 13.5 % Show Material materials with Silicona of 11.0 - 13.5 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |