General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Densidad | 20.0 °C | 2.75 g/cm³ Show Material materials with Densidad of 2.75 g/cm³ | T5 | DIN 1725-2, EN 1676, EN 1706 |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Elongación | 220.0 °C | 8.4 % Show Material materials with Elongación of 8.4 % | T5 | DIN 1725-2, EN 1676, EN 1706 | |
280.0 °C | 21.8 % Show Material materials with Elongación of 21.8 % | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Módulo elástico | 20.0 °C | 75.0 GPa Show Material materials with Módulo elástico of 75.0 GPa | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Resistencia a la tracción | 20.0 °C | 348.0 MPa Show Material materials with Resistencia a la tracción of 348.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | |
220.0 °C | 133.0 MPa Show Material materials with Resistencia a la tracción of 133.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
280.0 °C | 66.0 MPa Show Material materials with Resistencia a la tracción of 66.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 20.0 °C | 880.0 J/(kg·K) Show Material materials with Calor específico of 880.0 J/(kg·K) | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Coeficiente de dilatación térmica | 200.0 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Conductividad térmica | 20.0 °C | 110.0 - 130.0 W/(m·K) Show Material materials with Conductividad térmica of 110.0 - 130.0 W/(m·K) | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 14000000.0 - 18000000.0 S/m Show Material materials with Conductividad eléctrica of 14000000.0 - 18000000.0 S/m | T5 | DIN 1725-2, EN 1676, EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 82.1 % Show Material materials with Aluminio of 82.1 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Cobre | 2.0 - 3.5 % Show Material materials with Cobre of 2.0 - 3.5 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Estaño | 0.1 Show Material materials with Estaño of 0.1 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Hierro | 0.8 Show Material materials with Hierro of 0.8 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Manganeso | 0.1 - 0.5 % Show Material materials with Manganeso of 0.1 - 0.5 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Níquel | 0.3 Show Material materials with Níquel of 0.3 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Plomo | 0.2 Show Material materials with Plomo of 0.2 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Silicona | 8.0 - 11.0 % Show Material materials with Silicona of 8.0 - 11.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Titanio | 0.15 Show Material materials with Titanio of 0.15 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Zinc | 1.2 Show Material materials with Zinc of 1.2 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting |