General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Densidad | 20.0 °C | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | F | DIN 1725-2, EN 1676, EN 1706 |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Dureza Brinell | 20.0 °C | 45.0 [-] Show Material materials with Dureza Brinell of 45.0 [-] | F | DIN 1725-2, EN 1676, EN 1706 | |
20.0 °C | 50.0 [-] Show Material materials with Dureza Brinell of 50.0 [-] | F | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 50.0 - 65.0 [-] Show Material materials with Dureza Brinell of 50.0 - 65.0 [-] | F | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 50.0 - 60.0 [-] Show Material materials with Dureza Brinell of 50.0 - 60.0 [-] | F | DIN 1725-2, EN 1676, EN 1706 | ||
Elongación | 20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | F | DIN 1725-2, EN 1676, EN 1706 | |
20.0 °C | 3.0 - 8.0 % Show Material materials with Elongación of 3.0 - 8.0 % | F | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | F | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 4.0 - 10.0 % Show Material materials with Elongación of 4.0 - 10.0 % | F | DIN 1725-2, EN 1676, EN 1706 | ||
Módulo elástico | 20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | F | DIN 1725-2, EN 1676, EN 1706 | |
Resistencia a la tracción | 20.0 °C | 130.0 MPa Show Material materials with Resistencia a la tracción of 130.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 | |
20.0 °C | 140.0 MPa Show Material materials with Resistencia a la tracción of 140.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 140.0 - 190.0 MPa Show Material materials with Resistencia a la tracción of 140.0 - 190.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 | ||
20.0 °C | 150.0 - 200.0 MPa Show Material materials with Resistencia a la tracción of 150.0 - 200.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 | ||
Resistencia al cizallamiento | 20.0 °C | 146.0 MPa Show Material materials with Resistencia al cizallamiento of 146.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 20.0 °C | 930.0 J/(kg·K) Show Material materials with Calor específico of 930.0 J/(kg·K) | F | DIN 1725-2, EN 1676, EN 1706 | |
Coeficiente de dilatación térmica | 200.0 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | F | DIN 1725-2, EN 1676, EN 1706 | |
Conductividad térmica | 20.0 °C | 110.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 110.0 - 140.0 W/(m·K) | F | DIN 1725-2, EN 1676, EN 1706 | |
Temperatura de fusión | 450.0 - 640.0 °C Show Material materials with Temperatura de fusión of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 15000000.0 - 21000000.0 S/m Show Material materials with Conductividad eléctrica of 15000000.0 - 21000000.0 S/m | F | DIN 1725-2, EN 1676, EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 93.8 % Show Material materials with Aluminio of 93.8 % | F | DIN 1725-2, EN 1676, EN 1706 |
Cobre | 0.05 Show Material materials with Cobre of 0.05 | F | DIN 1725-2, EN 1676, EN 1706 |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | F | DIN 1725-2, EN 1676, EN 1706 |
Magnesio | 2.5 - 3.5 % Show Material materials with Magnesio of 2.5 - 3.5 % | F | DIN 1725-2, EN 1676, EN 1706 |
Manganeso | 0.001 - 0.4 % Show Material materials with Manganeso of 0.001 - 0.4 % | F | DIN 1725-2, EN 1676, EN 1706 |
Silicona | 0.9 - 1.3 % Show Material materials with Silicona of 0.9 - 1.3 % | F | DIN 1725-2, EN 1676, EN 1706 |
Titanio | 0.001 - 0.2 % Show Material materials with Titanio of 0.001 - 0.2 % | F | DIN 1725-2, EN 1676, EN 1706 |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | F | DIN 1725-2, EN 1676, EN 1706 |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting, sample taken from casting |