General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 2.705 g/cm³ Show Material materials with Densidad of 2.705 g/cm³ | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||
Módulo de cizallamiento | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | ||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 900.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium | |||
Coeficiente de dilatación térmica | 20 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | ||
Conductividad térmica | 230.0 - 234.0 W/(m·K) Show Material materials with Conductividad térmica of 230.0 - 234.0 W/(m·K) | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | ||
Temperatura de fusión | 645.0 - 655.0 °C Show Material materials with Temperatura de fusión of 645.0 - 655.0 °C | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Eléctrico
Property | Value | Related Standards | Shape |
---|---|---|---|
Conductividad eléctrica | 35000000.0 - 36000000.0 S/m Show Material materials with Conductividad eléctrica of 35000000.0 - 36000000.0 S/m | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Resistividad eléctrica | 2.78e-08 - 2.86e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.78e-08 - 2.86e-08 Ω·m | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 99.6 % Show Material materials with Aluminio of 99.6 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % | EN 573-3 | |
0.35 % Show Material materials with Hierro of 0.35 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
Magnesio | 0.03 % Show Material materials with Magnesio of 0.03 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Manganeso | 0.03 % Show Material materials with Manganeso of 0.03 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |