General
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Elongación | 25.0 % Show Material materials with Elongación of 25.0 % | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | ||
29.0 % Show Material materials with Elongación of 29.0 % | O | EN 573-3 | Strip, Sheet, Plate | |||
30.0 % Show Material materials with Elongación of 30.0 % | O | EN 573-3 | Strip, Sheet, Plate | |||
33.0 % Show Material materials with Elongación of 33.0 % | O | EN 573-3 | Strip, Sheet, Plate | |||
20.0 °C | 25.0 % Show Material materials with Elongación of 25.0 % | O | EN 573-3 | Wire | A100 | |
20.0 °C | 29.0 % Show Material materials with Elongación of 29.0 % | O | EN 573-3 | Rod | ||
20.0 °C | 30.0 % Show Material materials with Elongación of 30.0 % | O | EN 573-3 | Sheet, Strip | ||
20.0 °C | 33.0 % Show Material materials with Elongación of 33.0 % | O | EN 573-3 | Sheet, Strip | ||
Módulo de cizallamiento | 20.0 °C | 25.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 25.0 - 26.5 GPa | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
Módulo elástico | -270 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | |
-270.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |||
20 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
20.0 °C | 70.0 - 72.0 GPa Show Material materials with Módulo elástico of 70.0 - 72.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
20.0 °C | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | O | EN 573-3 | Wire | ||
50.0 °C | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
100.0 °C | 68.0 GPa Show Material materials with Módulo elástico of 68.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
150.0 °C | 66.0 GPa Show Material materials with Módulo elástico of 66.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
200.0 °C | 63.0 GPa Show Material materials with Módulo elástico of 63.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
250.0 °C | 57.0 GPa Show Material materials with Módulo elástico of 57.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
300 °C | 50.0 GPa Show Material materials with Módulo elástico of 50.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
300.0 °C | 50.0 GPa Show Material materials with Módulo elástico of 50.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Resistencia a la tracción | 40.0 MPa Show Material materials with Resistencia a la tracción of 40.0 MPa | O | EN 573-3 | Strip, Sheet, Plate | ||
70.0 MPa Show Material materials with Resistencia a la tracción of 70.0 MPa | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |||
20.0 °C | 40.0 MPa Show Material materials with Resistencia a la tracción of 40.0 MPa | O | EN 573-3 | Rod, Sheet, Strip | ||
20.0 °C | 70.0 MPa Show Material materials with Resistencia a la tracción of 70.0 MPa | O | EN 573-3 | Wire |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20.0 °C | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
Coeficiente de dilatación térmica | -50 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire |
-50.0 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
20 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
20 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
20 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
100 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
100.0 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
200 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
200.0 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
300 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
300.0 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
Conductividad térmica | 232 W/(m·K) Show Material materials with Conductividad térmica of 232 W/(m·K) | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20.0 °C | 215.0 - 227.0 W/(m·K) Show Material materials with Conductividad térmica of 215.0 - 227.0 W/(m·K) | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
Temperatura de fusión | 660.0 °C Show Material materials with Temperatura de fusión of 660.0 °C | O | EN 573-3, EN 1301 | Strip, Sheet, Plate |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 37500000.0 - 37700000.0 S/m Show Material materials with Conductividad eléctrica of 37500000.0 - 37700000.0 S/m | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20.0 °C | 37600000.0 - 37800000.0 S/m Show Material materials with Conductividad eléctrica of 37600000.0 - 37800000.0 S/m | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
Resistividad eléctrica | 2.65e-08 - 2.67e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.65e-08 - 2.67e-08 Ω·m | O | EN 573-3, EN 1301 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 99.98 % Show Material materials with Aluminio of 99.98 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Cobre | 0.003 % Show Material materials with Cobre of 0.003 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Hierro | 0.006 % Show Material materials with Hierro of 0.006 % | O | EN 573-3 | Rod, Sheet, Strip, Wire |
0.006 % Show Material materials with Hierro of 0.006 % | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Titanio | 0.003 % Show Material materials with Titanio of 0.003 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Zinc | 0.015 % Show Material materials with Zinc of 0.015 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good, general: very good | |
Corrosion properties | Seawater: acceptable, weathering: good | |
Workability | Bending / Spinning (cold): very good |