General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H111 | EN 573-3, EN 1386, EN 485 | Strip, Sheet, Plate |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Elongación | 5.0 % Show Material materials with Elongación of 5.0 % | H111 | EN 573-3, EN 1386 | Strip, Sheet, Plate | A50 | |
6.0 % Show Material materials with Elongación of 6.0 % | H111 | EN 573-3, EN 1386, EN 485 | Strip, Sheet, Plate | A100 | ||
9.0 % Show Material materials with Elongación of 9.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
10.0 % Show Material materials with Elongación of 10.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
11.0 % Show Material materials with Elongación of 11.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
12.0 % Show Material materials with Elongación of 12.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | A50 | ||
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H111 | EN 573-3 | Plate | A50 | |
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | H111 | EN 573-3 | Plate, Sheet | ||
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | H111 | EN 573-3 | Sheet | ||
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | H111 | EN 573-3 | Sheet | ||
20.0 °C | 11.0 % Show Material materials with Elongación of 11.0 % | H111 | EN 573-3 | Flat | Transverse | |
20.0 °C | 11.0 % Show Material materials with Elongación of 11.0 % | H111 | EN 573-3 | Flat | ||
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | H111 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | H111 | EN 573-3 | Flat | A50 | |
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Módulo elástico | 69.0 - 70.0 GPa Show Material materials with Módulo elástico of 69.0 - 70.0 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | H111 | EN 573-3, EN 1386 | Strip, Sheet, Plate | ||
20.0 °C | 200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | H111 | EN 573-3 | Plate | ||
20.0 °C | 210.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 300.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 210.0 - 285.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 285.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 210.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 270.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 210.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 270.0 MPa | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 210.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 300.0 MPa | H111 | EN 573-3 | Sheet | ||
20.0 °C | 210.0 - 285.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 285.0 MPa | H111 | EN 573-3 | Sheet | ||
20.0 °C | 230.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 300.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 230.0 - 285.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 285.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 230.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 270.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 230.0 - 285.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 285.0 MPa | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 230.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 300.0 MPa | H111 | EN 573-3 | Sheet | ||
20.0 °C | 230.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 230.0 - 270.0 MPa | H111 | EN 573-3 | Sheet | ||
20.0 °C | 245.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 245.0 - 300.0 MPa | H111 | EN 573-3 | Sheet, Flat | Transverse | |
20.0 °C | 245.0 - 285.0 MPa Show Material materials with Resistencia a la tracción of 245.0 - 285.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 245.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 245.0 - 270.0 MPa | H111 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 245.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 245.0 - 300.0 MPa | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Flat | ||
20.0 °C | 245.0 - 285.0 MPa Show Material materials with Resistencia a la tracción of 245.0 - 285.0 MPa | H111 | EN 573-3 | Sheet | ||
20.0 °C | 245.0 - 270.0 MPa Show Material materials with Resistencia a la tracción of 245.0 - 270.0 MPa | H111 | EN 573-3 | Sheet |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 879.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium |
Coeficiente de dilatación térmica | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium |
Conductividad térmica | 112.0 - 205.0 W/(m·K) Show Material materials with Conductividad térmica of 112.0 - 205.0 W/(m·K) | Typical for Wrought 5000 Series Aluminium |
Temperatura de fusión | 560.0 - 655.0 °C Show Material materials with Temperatura de fusión of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium |
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 31000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
Resistividad eléctrica | 3.3e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Circonio | 0.3 % Show Material materials with Circonio of 0.3 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Cobre | 0.1 - 0.8 % Show Material materials with Cobre of 0.1 - 0.8 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Hierro | 0.2 - 1.0 % Show Material materials with Hierro of 0.2 - 1.0 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Magnesio | 3.9 - 4.9 % Show Material materials with Magnesio of 3.9 - 4.9 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Manganeso | 0.6 - 1.8 % Show Material materials with Manganeso of 0.6 - 1.8 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Silicona | 0.55 - 1.4 % Show Material materials with Silicona of 0.55 - 1.4 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Zinc | 1.0 % Show Material materials with Zinc of 1.0 % | H111 | EN 573-3, EN 1386, EN 485 | Sheet, Flat, Plate, Strip |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |