General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Dureza Brinell | 60.0 [-] Show Material materials with Dureza Brinell of 60.0 [-] | T7 | EN 1706 | Casting | |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Resistencia a la tracción | 200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | T7 | EN 1706 | Casting |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T7 | EN 1706 | Casting | |
100 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T7 | EN 1706 | Casting | ||
Conductividad térmica | 140.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 - 170.0 W/(m·K) | T7 | EN 1706 | Casting | ||
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 19000000.0 - 25000000.0 S/m Show Material materials with Conductividad eléctrica of 19000000.0 - 25000000.0 S/m | T7 | EN 1706 | Casting |
Resistividad eléctrica | 4e-08 - 5.26e-08 Ω·m Show Material materials with Resistividad eléctrica of 4e-08 - 5.26e-08 Ω·m | T7 | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 86.38 % Show Material materials with Aluminio of 86.38 % | T7 | EN 1706 | |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | T7 | EN 1706 | Casting |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % | T7 | EN 1706 | |
0.25 % Show Material materials with Hierro of 0.25 % | T7 | EN 1706 | Casting | |
Magnesio | 0.1 - 0.6 % Show Material materials with Magnesio of 0.1 - 0.6 % | T7 | EN 1706 | Casting |
Manganeso | 0.4 - 0.8 % Show Material materials with Manganeso of 0.4 - 0.8 % | T7 | EN 1706 | Casting |
Silicona | 9.0 - 11.5 % Show Material materials with Silicona of 9.0 - 11.5 % | T7 | EN 1706 | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | T7 | EN 1706 | Casting |
Zinc | 0.07 % Show Material materials with Zinc of 0.07 % | T7 | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: good | |
General machinability | after thermal treatment: good, as cast: good to acceptable | |
Processing methods | pressure die casting, separately cast test sample |