Description

Related Standards

Properties

Mechanical

Elongation A

40 % at 20 °C

Tensile strength Rm

690 MPa at 20 °C

Yield strength YS

283 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Ni

-

REM

Mo

16 %

Cr

15.5 %

Fe

5 %

W

4 %