EFI Alloy 50 Square Bar

Alternative and trade names
Magnifer 50®, Carpenter High Permeability 49®, Alloy 47-50
.XLSX
.PDF
Save

Description

A soft magnetic alloy, consisting of 48% nickel, balance iron used where high initial permeability, maximum permeability, and low core loss is needed.

Related Standards

Equivalent Materials

Properties

General

Density ρ

8.18 g/cm³ at 20 °C

Dimension

Dimensions

Available widths: 26.16mm, 51.56mm

Length l

3050 - 3660 mm

Mill random length

Width w

26.2 - 51.6 mm

Mechanical

Elastic modulus E

166 GPa at 20 °C

Elongation A

40 % at 20 °C

in 2 in.

Hardness, Rockwell B HRB

80 [-] at 20 °C

Tensile strength Rm

518 MPa at 20 °C

Yield strength YS

159 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

9E-6 1/K at 450 °C

Melting point Tm

1427 °C

Specific heat capacity cp

502 J/(kg·K) at 20 °C

Thermal conductivity λ

13 W/(m·K) at 20 °C

Electrical

Electrical resistivity ρel

4.9E-7 Ω·m at 20 °C

Magnetic

Coercive force Hc

4.77 A/m at 20 °C

Curie temperature Tc

450 °C

Relative magnetic permeability μrel

100000 [-] at 20 °C

Saturation induction Bs

1.5 T at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

-

Balance

Ni

48 %

Mn

0.5 %

Si

0.35 %

C

0.02 %

Technological properties

Application areas

Common applications of EFI ALLOY 50 are: LF power transducers, stepping motors, magnetic shielding, solenoid cores, relay parts, magnetic valves

This material data has been provided by Ed Fagan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.