Description

A controlled expansion alloy, consisting of 51% Nickel, balance Iron.

Related Standards

Equivalent Materials

Properties

General

Density ρ

8.3 g/cm³ at 20 °C

Dimension

Dimensions

Available thicknesses: 0.254mm, 0.381mm

Thickness t

0.25 - 0.38 mm

Mechanical

Elastic modulus E

159 GPa at 20 °C

Elongation A

35 % at 20 °C

in 2 in.

Hardness, Rockwell B HRB

80 [-] at 20 °C

Tensile strength Rm

552 MPa at 20 °C

Yield strength YS

276 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.05E-5 1/K at 100 °C

Show chart

Melting point Tm

1427 °C

Specific heat capacity cp

502 J/(kg·K) at 20 °C

Thermal conductivity λ

14 W/(m·K) at 20 °C

Electrical

Electrical resistivity ρel

4.4E-7 Ω·m at 20 °C

Magnetic

Curie temperature Tc

530 °C

Chemical properties

Element

Weight %

Comment

Fe

-

Balance

Ni

50.5 %

Si

0.3 %

C

0.05 %

Cr

0.03 %

More

Technological properties

Application areas

Common applications of Alloy 52: Pin feed-throughs for semiconductor devices, glass-to-metal sealing with soft glass for mercury switches and semiconductor devices

This material data has been provided by Ed Fagan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.