StarCeram® N7000 Silicon Nitride (Si₃N₄)

.XLSX
.PDF
Save

Description

The key benefits of StarCeram® N include: Extremely high strength even up to >1200°C, excellent wear and chipping resistance, high hardness, high fracture toughness, low thermal expansion, average thermal conductivity, very good thermal shock resistance, very good chemical resistance, electrically conductive material available.

Properties

Electrical

Electrical resistivity ρel

1.00E+11 - 1.00E+12 Ω·m at 20 °C

General

Density ρ

3.22 g/cm³ at 20 °C

Mechanical

Elastic modulus E

290 GPa at 20 °C

Flexural strength σbend

800 MPa at 20 °C

4-point bending, 40/20mm

Fracture toughness KIC

6.7 MPa·√m at 20 °C

Hardness, Vickers HV

1530 [-] at 20 °C

converted from 15 GPa

Weibull modulus mW

15 [-] at 20 °C

min

Thermal

Coefficient of thermal expansion α

3.4E-6 1/K at 20 °C

RT - 1000°C

Max service temperature Tmax

1000 °C

Thermal conductivity λ

20 W/(m·K) at 20 °C

Thermal shock parameter R1 R1

620 °C

Technological properties

Application areas

Bearing bushes, protection sleeves, crucibles, cylinder linings, dosing tubes, riser tubes, extruder screws, forming rolls, guide rolls, immersion heater tubes, mill linings, nozzles, slide valves, rotors, sliding rings, thermo protection tubes, thermocouple protection tubes, wear protection parts, welding rolls, centering pins

This material data has been provided by KYOCERA Fineceramics Precision GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.