VT 8-1 (Ti-6Al-3Mo-1Zr-1Sn) Bar

.XLSX
.PDF
Save

Description

Equivalent Materials

Properties

Dimension

Diameter d

7 - 115 mm

Length l

6000 mm

max

Material Information

Dimension

7-14.5 mm diameter up to 3000 mm length; 15-65 mm diameter up to 6000 mm length; 66-115 mm diameter up to 5000 mm length.

Chemical properties

Element

Weight %

Comment

Al

5.8 - 6.8 %

Mo

2.8 - 3.8 %

Zr

0.5 - 1.5 %

Fe

0.2 %

O

0.15 %

More

This material data has been provided by VSMPO.