VT 1-0 Tubular Billet

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

General

Density ρ

4.51 g/cm³ at 20 °C

Dimension

Diameter d

25.4 - 125 mm

Wall thickness

2.5 - 21 mm

Mechanical

Elongation A

10 - 30 % at 20 °C

Tensile strength Rm

295 - 590 MPa at 20 °C

Thermal

Melting point Tm

1668 °C

Specific heat capacity cp

540 J/(kg·K) at 20 °C

Thermal conductivity λ

18.85 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

0.25 %

O

0.2 %

Si

0.1 %

C

0.07 %

N

0.04 %

More

This material data has been provided by VSMPO.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.