Properties

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

9.9E-8 - 1.01E-7 Ω·m

Show Material materials with Electrical resistivity of 9.9E-8 - 1.01E-7 Ω·m

General

PropertyTemperatureValue

Density

20.0 °C

12 g/cm³

Show Material materials with Density of 12 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

-195.0 °C

126 GPa

Show Material materials with Elastic modulus of 126 GPa

20.0 °C

121 - 124 GPa

Show Material materials with Elastic modulus of 121 - 124 GPa

250.0 °C

121 GPa

Show Material materials with Elastic modulus of 121 GPa

400.0 °C

119 GPa

Show Material materials with Elastic modulus of 119 GPa

500.0 °C

117 GPa

Show Material materials with Elastic modulus of 117 GPa

600.0 °C

113 GPa

Show Material materials with Elastic modulus of 113 GPa

750.0 °C

98 GPa

Show Material materials with Elastic modulus of 98 GPa

800.0 °C

91 GPa

Show Material materials with Elastic modulus of 91 GPa

Elongation

20.0 °C

16 - 94 %

Show Material materials with Elongation of 16 - 94 %

Hardness, Vickers

20.0 °C

9 - 140 [-]

Show Material materials with Hardness, Vickers of 9 - 140 [-]

Tensile strength

20.0 °C

9 - 440 MPa

Show Material materials with Tensile strength of 9 - 440 MPa

Yield strength Rp0.2

20.0 °C

5 - 340 MPa

Show Material materials with Yield strength Rp0.2 of 5 - 340 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

50.0 °C

1.18E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.18E-5 1/K

100.0 °C

1.19E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K

200.0 °C

1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K

300.0 °C

1.23E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.23E-5 1/K

400.0 °C

1.26E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.26E-5 1/K

500.0 °C

1.28E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K

600.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

700.0 °C

1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K

800.0 °C

1.34E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.34E-5 1/K

900.0 °C

1.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K

1000.0 °C

1.39E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K

Unlock all property charts

Melting point

1552 °C

Show Material materials with Melting point of 1552 °C

Thermal conductivity

-173.0 °C

76 W/(m·K)

Show Material materials with Thermal conductivity of 76 W/(m·K)

-73.0 °C

75 W/(m·K)

Show Material materials with Thermal conductivity of 75 W/(m·K)

0.0 °C

75.1 W/(m·K)

Show Material materials with Thermal conductivity of 75.1 W/(m·K)

20.0 °C

75 W/(m·K)

Show Material materials with Thermal conductivity of 75 W/(m·K)

127.0 °C

75.5 W/(m·K)

Show Material materials with Thermal conductivity of 75.5 W/(m·K)

327.0 °C

79 W/(m·K)

Show Material materials with Thermal conductivity of 79 W/(m·K)

527.0 °C

83 W/(m·K)

Show Material materials with Thermal conductivity of 83 W/(m·K)

727.0 °C

87 W/(m·K)

Show Material materials with Thermal conductivity of 87 W/(m·K)

927.0 °C

88.2 W/(m·K)

Show Material materials with Thermal conductivity of 88.2 W/(m·K)

1127.0 °C

86.9 W/(m·K)

Show Material materials with Thermal conductivity of 86.9 W/(m·K)

1327.0 °C

86 W/(m·K)

Show Material materials with Thermal conductivity of 86 W/(m·K)

Unlock all property charts

Chemical properties

PropertyValue

Palladium

99.9 %

Show Material materials with Palladium of 99.9 %