The material: 'Cu-HCP / DD14 / Cu-HCP (55-40-5)' you were looking for has been superseded by the one below.

Cu-HCP / DD14 / Cu-HCP (55-40-5)

Alternative and trade names
CUFER 2
Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.5 g/cm³

Show Material materials with Density of 8.5 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

157 GPa

Show Material materials with Elastic modulus of 157 GPa

Tensile strength

23.0 °C

268 MPa

Show Material materials with Tensile strength of 268 MPa

Yield strength

23.0 °C

146 MPa

Show Material materials with Yield strength of 146 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.35E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.35E-5 1/K

Coefficient of thermal expansion, transverse

23.0 °C

0.02 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 0.02 1/K

Specific heat capacity

23.0 °C

414.54 J/(kg·K)

Show Material materials with Specific heat capacity of 414.54 J/(kg·K)

Thermal conductivity

23.0 °C

253 W/(m·K)

Show Material materials with Thermal conductivity of 253 W/(m·K)

Thermal conductivity, through-plane

23.0 °C

113.24 W/(m·K)

Show Material materials with Thermal conductivity, through-plane of 113.24 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

3.81E+7 S/m

Show Material materials with Electrical conductivity of 3.81E+7 S/m

Electrical conductivity, transverse

23.0 °C

1.43E+7 S/m

Show Material materials with Electrical conductivity, transverse of 1.43E+7 S/m

Electrical resistivity

23.0 °C

2.6E-8 Ω·m

Show Material materials with Electrical resistivity of 2.6E-8 Ω·m

Technological properties

Property
Coating

Different coating layers are available upon request.